IRON DISSOLUTION AND PASSIVATION IN K2CO3-KHCO3 SOLUTIONS - ROTATING-RING-DISK ELECTRODE AND XPS STUDIES

被引:98
作者
CASTRO, EB
VILCHE, JR
ARVIA, AJ
机构
[1] Instituto de Investigaciones Fisicoquimicas Teóricas y Aplicadas (INIFTA), Facultad de Ciencias Exactas, Universidad Nacional de La Plata, 1900 La Plata, Sucursal 4
关键词
D O I
10.1016/0010-938X(91)90062-T
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Rotating ring-disc electrode studies on the anodic dissolution and passivation of iron in potassium carbonate/bicarbonate buffers at 25°C show that in the active anodic dissolution potential range Fe(II) soluble species are generated. This reaction is favoured by the presence of bicarbonate ions in solution and it is explained through the formation of an unstable soluble complex containing Fe(II) and HCO-3 ions. This suggests that the anodic layer at a certain stage of its formation contains some amount of carbonate species. XPS data of surface layers produced at different anodic potentials confirm the presence of the carbonate species in thick anodic layers grown in the prepassive potential region in still solutions, whereas the opposite result is found for the thin passive layers formed at high positive potentials. © 1991.
引用
收藏
页码:37 / 50
页数:14
相关论文
共 41 条
[1]   A COMPARATIVE ELECTROCHEMICAL AND ELLIPSOMETRIC STUDY OF IRON ELECTRODES IN DIFFERENT ALKALINE ELECTROLYTES [J].
ALBANI, OA ;
ZERBINO, JO ;
VILCHE, JR ;
ARVIA, AJ .
ELECTROCHIMICA ACTA, 1986, 31 (11) :1403-1411
[2]   PASSIVATION OF IRON IN CARBONATE-BICARBONATE SOLUTIONS [J].
ARMSTRONG, RD ;
COATES, AC .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1974, 50 (03) :303-313
[3]   SPECTROSCOPIC OBSERVATIONS ON THE NATURE OF PASSIVITY [J].
BOCKRIS, JO .
CORROSION SCIENCE, 1989, 29 (2-3) :291-312
[4]  
BRIGGS D, 1983, PRACTICAL SURFACE AN
[5]  
BRINDAKONOPIK N, 1982, DECHEMA MONOGR, V92, P207
[6]  
Brusic V., 1972, OXIDES OXIDE FILMS, P1
[7]  
Carlson T. A., 1975, PHOTOELECTRON AUGER
[8]  
CASTRO BE, 1987, 10TH P INT C MET COR, P2071
[9]   THE INFLUENCE OF IONIC COMPOSITION ON THE ELECTRODISSOLUTION AND PASSIVATION OF IRON ELECTRODES IN POTASSIUM CARBONATE BICARBONATE SOLUTIONS IN THE 8.4-10.5 PH RANGE AT 25-DEGREES-C [J].
CASTRO, EB ;
VALENTINI, CR ;
MOINA, CA ;
VILCHE, JR ;
ARVIA, AJ .
CORROSION SCIENCE, 1986, 26 (10) :781-&
[10]   CATHODIC REDUCTION OF GAMMA-FEOOH, GAMMA-FE2O3, AND OXIDE-FILMS ON IRON [J].
COHEN, M ;
HASHIMOTO, K .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1974, 121 (01) :42-45