The solidification of toxic waste using OPC is practiced in a number of countries. OPC is known to interreact with some waste components. PFA is often added as a cement replacement material on grounds of cost and so that the final properties of solidified waste are improved. An inorganic waste, typical of that solidified commercially, has been shown by isothermal conduction calorimetry, strength development and microstructural studies to markedly influence the early hydration of OPC. PFA was shown to contribute to strength development under conditions where the OPC hydration reaction was almost completely poisoned.
引用
收藏
页码:822 / 832
页数:11
相关论文
共 14 条
[1]  
Conner JR., 1990, CHEM FIXATION SOLIDI
[2]   ORGANIC INTERFERENCE OF SOLIDIFIED STABILIZED HAZARDOUS WASTES [J].
EATON, HC ;
WALSH, MB ;
TITTLEBAUM, ME ;
CARTLEDGE, FK ;
CHALASANI, D .
ENVIRONMENTAL MONITORING AND ASSESSMENT, 1987, 9 (02) :133-142
[3]  
Jawed I., 1983, STRUCTURE PERFORMANC
[4]  
JONES LW, 1988, USEPA DW219306080010
[5]   REACTIONS OF SOME CALCIUM SILICATES WITH METAL-CATIONS [J].
KOMARNENI, S ;
BREVAL, E ;
ROY, DM ;
ROY, R .
CEMENT AND CONCRETE RESEARCH, 1988, 18 (02) :204-220
[6]  
Minnick L. J., 1967, P FLY ASH UT C AM PU, P287
[7]   MECHANISMS OF METAL FIXATION AND LEACHING BY CEMENT BASED FIXATION PROCESSES [J].
POON, CS ;
CLARK, AI ;
PETERS, CJ ;
PERRY, R .
WASTE MANAGEMENT & RESEARCH, 1985, 3 (02) :127-142
[8]  
PORTEOUS A, 1985, HAZARDOUS WASTE MANA
[9]  
SCRIVENER KL, 1989, MATERIALS SCI CONCRE
[10]   HARDENING PROPERTY OF CEMENT MORTAR ADDING HEAVY-METAL COMPOUND AND SOLUBILITY OF HEAVY-METAL FROM HARDENED MORTAR [J].
TASHIRO, C ;
TAKAHASHI, H ;
KANAYA, M ;
HIRAKIDA, I ;
YOSHIDA, R .
CEMENT AND CONCRETE RESEARCH, 1977, 7 (03) :283-290