INFLUENCE OF MICROSTRUCTURE ON FRACTURE OF DRAWN TUNGSTEN WIRE

被引:36
作者
FUNKENBUSCH, AW
BACON, F
LEE, D
机构
[1] GE,RES & DEV,MET LAB,SCHENECTADY,NY 12301
[2] GE,DEPT REFRACTORY MET PROD,SCHENECTADY,NY 12301
[3] GE,RES & DEV,MAT CHARACTERIZAT LAB,SCHENECTADY,NY 12301
来源
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE | 1979年 / 10卷 / 08期
关键词
D O I
10.1007/BF02811654
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructures and longitudinal fracture resistances of 0.635 mm diam lamp-doped and undoped tungsten wire were examined in the as-drawn condition and after anealing at temperatures between 600 and 1500°C. A variety of experimental techniques were employed, including Auger Electron Spectroscopy, Scanning Electron Microscopy, Transmission Electron Microscopy and a newly developed mechanical testing technique. The longitudinal fracture mode was intergranular for all wires and a second phase was observed on the grain boundaries of all doped wires. High concentrations of the dopant element potassium were present on the fracture surfaces of doped wires and experimental evidence was obtained which suggests they may be due to postfracture surface diffusion. Doped wires demonstrated increasing amounts of structure coarsening up to 1500°C whereas large equiaxed grains were formed in undoped wires annealed at 1300 and 1500°C. The longitudinal fracture resistance of undoped wire was unaltered by annealing at 1050°C and below, but decreased dramatically after annealing at 1300 and 1500°C. In contrast the fracture resistance of doped wire decreased after annealing at 1050 and 1300°C, but increased after annealing at 1500°C. Fracture resistance is discussed in terms of microstructure and fracture surface chemistry. © 1979 American Society for Metals and the Metallurgical Society of AIME.
引用
收藏
页码:1085 / 1091
页数:7
相关论文
共 16 条
[1]  
ATKINSON RH, 1962, REFRACTORY METALS AL, V17, P319
[2]  
Davies L.E., 1976, HDB AUGER ELECTRON S, P5
[3]  
HAHN GT, 1962, REFRACTORY METALS AL, V17, P23
[4]  
HUNTZ AM, 1971, MET, V46, P545
[5]  
JONES DJ, 1973, METALLURGIST MATER T, V5, P503
[6]   FRACTURE OF DRAWN TUNGSTEN WIRES [J].
LEE, D .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1975, 6 (11) :2083-2088
[7]  
MEIRAN ES, 1965, T TMS AIME, V233, P937
[8]   MECHANISM AND KINETICS OF BUBBLE FORMATION IN DOPED TUNGSTEN [J].
MOON, DM ;
KOO, RC .
METALLURGICAL TRANSACTIONS, 1971, 2 (08) :2115-&
[9]  
PEBLER A, 1975, METALL TRANS, VA 6, P991, DOI 10.1007/BF02661351
[10]   ADSORPTION OF POTASSIUM ON TUNGSTEN [J].
SCHMIDT, L ;
GOMER, R .
JOURNAL OF CHEMICAL PHYSICS, 1965, 42 (10) :3573-&