In Vitro Evaluation of Bioactivity of Chemically Deposited Hydroxyapatite on Polyether Ether Ketone

被引:8
作者
Almasi, D. [1 ,2 ]
Izman, S. [1 ]
Sadeghi, M. [3 ]
Iqbal, N. [2 ]
Roozbahani, F. [4 ]
Krishnamurithy, G. [5 ,6 ]
Kamarul, T. [6 ]
Kadir, M. R. Abdul [2 ]
机构
[1] Univ Teknol Malaysia, Fac Mech Engn, Dept Mfg & Ind Engn, Skudai 81310, Johor, Malaysia
[2] Univ Teknol Malaysia, Fac Biosci & Med Engn, Med Devices & Technol Grp MEDITEG, Skudai 81310, Johor, Malaysia
[3] Univ Teknol Malaysia, Fac Chem Engn, Johor Baharu 81310, Johor, Malaysia
[4] Univ Teknol Malaysia, Fac Biosci & Med Engn, Skudai 81310, Johor, Malaysia
[5] Univ Liverpool, Inst Translat Med, Liverpool L69 3GE, Merseyside, England
[6] Univ Malaya, Fac Med, NOCERAL, Dept Orthopaed Surg, Kuala Lumpur 50603, Malaysia
关键词
D O I
10.1155/2015/475435
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 [材料科学与工程]; 080501 [材料物理与化学]; 080502 [材料学];
摘要
Polyether ether ketone (PEEK) is considered the best alternative material for titanium for spinal fusion cage implants due to its low elasticity modulus and radiolucent property. The main problem of PEEK is its bioinert properties. Coating with hydroxyapatite (HA) showed very good improvement in bioactivity of the PEEK implants. However the existing methods for deposition of HA have some disadvantages and damage the PEEK substrate. In our previous study a new method for deposition of HA on PEEK was presented. In this study cell proliferation of mesenchymal stem cell and apatite formation in simulated body fluid (SBF) tests were conducted to probe the effect of this new method in improvement of the bioactivity of PEEK. The mesenchymal stem cell proliferation result showed better cells proliferation on the treated layer in comparison with untreated PEEK. The apatite formation results showed the growth of the HA on the treated PEEK but there was not any sight of the growth of HA on the untreated PEEK even after 2 weeks. The results showed the new method of the HA deposition improved the bioactivity of the treated PEEK in comparison with the bare PEEK.
引用
收藏
页数:5
相关论文
共 10 条
[1]
Crystalline ha coating on peek via chemical deposition [J].
Almasi, D. ;
Izman, S. ;
Assadian, M. ;
Ghanbari, M. ;
Kadir, M. R. Abdul .
APPLIED SURFACE SCIENCE, 2014, 314 :1034-1040
[2]
Hengky C., 2008, P 13 INT C BIOM ENG, P261
[3]
How useful is SBF in predicting in vivo bone bioactivity? [J].
Kokubo, T ;
Takadama, H .
BIOMATERIALS, 2006, 27 (15) :2907-2915
[4]
Apatite formation on surfaces of ceramics, metals and polymers in body environment [J].
Kokubo, T .
ACTA MATERIALIA, 1998, 46 (07) :2519-2527
[5]
FATIGUE AND LIFETIME OF BIOACTIVE GLASS CERAMIC A-W CONTAINING APATITE AND WOLLASTONITE [J].
KOKUBO, T ;
ITO, S ;
SHIGEMATSU, M ;
SAKKA, S ;
YAMAMURO, T .
JOURNAL OF MATERIALS SCIENCE, 1987, 22 (11) :4067-4070
[6]
Characterization of bovine-derived porous hydroxyapatite scaffold and its potential to support osteogenic differentiation of human bone marrow derived mesenchymal stem cells [J].
Krishnamurithy, G. ;
Murali, Malliga Raman ;
Hamdi, M. ;
Abbas, A. A. ;
Raghavendran, Hanumantharao Balaji ;
Kamarul, T. .
CERAMICS INTERNATIONAL, 2014, 40 (01) :771-777
[7]
Osseointegration of machined, injection moulded and oxygen plasma modified PEEK implants in a sheep model [J].
Poulsson, Alexandra H. C. ;
Eglin, David ;
Zeiter, Stefan ;
Camenisch, Karin ;
Sprecher, Christoph ;
Agarwal, Yash ;
Nehrbass, Dirk ;
Wilson, Joanne ;
Richards, Robert G. .
BIOMATERIALS, 2014, 35 (12) :3717-3728
[8]
Processing and evaluation of bioactive coatings on polymeric implants [J].
Rabiei, Afsaneh ;
Sandukas, Stefan .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2013, 101 (09) :2621-2629
[9]
Laser surface modification of PEEK [J].
Riveiro, A. ;
Soto, R. ;
Comesana, R. ;
Boutinguiza, M. ;
del Val, J. ;
Quintero, F. ;
Lusquinos, F. ;
Pou, J. .
APPLIED SURFACE SCIENCE, 2012, 258 (23) :9437-9442
[10]
Strnad Z, 2000, INT J ORAL MAX IMPL, V15, P483