THERMAL DEGRADATION OF POLYFLUORAL AND METHODS OF STABILIZATION

被引:8
作者
BUSFIELD, WK
机构
[1] Department of Chemistry, University of Dundee, Scotland
关键词
D O I
10.1016/0032-3861(68)90058-X
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
The rates of thermal degradation of polymers of fluoral are reported. Both the thermal stability and the mechanism of degradation vary markedly according to the method of polymer preparation. In general the thermal stability is poor, one sample decomposing in 15 minutes at 120°C. Methods of stabilizing the polymer are described. After stabilization one sample did not degrade below 330°C. © 1968.
引用
收藏
页码:479 / &
相关论文
共 11 条
[1]  
BROWN F, 1952, J CHEM SOC, P5049
[2]   INFRARED SPECTRA AND STRUCTURE OF POLYALDEHYDES .6. POLYFLUORAL [J].
BUSFIELD, WK ;
WHALLEY, E .
CANADIAN JOURNAL OF CHEMISTRY, 1965, 43 (08) :2289-&
[3]  
BUSFIELD WK, 1966, POLYMER LOND, V71, P541
[4]  
IWASA Y, 1963, J CHEM SOC JAPAN PC, V84, P31
[5]  
Koch T.A., 1959, J APPL POLYM SCI, V1, P164
[6]   HYDRATES OF FLUORAL [J].
MCGREER, DE ;
MOCEK, MM ;
STEWART, R .
CANADIAN JOURNAL OF CHEMISTRY-REVUE CANADIENNE DE CHIMIE, 1963, 41 (04) :1024-&
[7]   POLY(CHLOROALDEHYDES) .I. POLYCHLORAL STABILIZATION [J].
ROSEN, I ;
HUDGIN, DE ;
STURM, CL ;
MCCAIN, GH ;
WILHJELM, RM .
JOURNAL OF POLYMER SCIENCE PART A-GENERAL PAPERS, 1965, 3 (4PA) :1535-&
[8]  
SHECHTER H, 1950, J AMER CHEM SOC, V74, P5422
[9]  
Wall L. A., 1962, RUBBER CHEM TECHNOL, V35, P1157
[10]  
1957, Patent No. 70717