OPTIMIZATION OF THE USE OF BASOLAN DC IN THE SHRINK-RESIST TREATMENT OF WOOL

被引:20
作者
JOVANCIC, P
JOCIC, D
TRAJKOVIC, R
DROBNJAK, S
机构
[1] Textile Engineering Department, University of Belgrade, Belgrade
关键词
17;
D O I
10.1080/00405009308631246
中图分类号
TB3 [工程材料学]; TS1 [纺织工业、染整工业];
学科分类号
0805 ; 080502 ; 0821 ;
摘要
The influence of Basolan DC applied by an exhaustion treatment on the changes in the mechanical and physico-chemical characteristics of wool fabric is studied by using a central composite rotatable design. The optimum conditions of the treatment are chosen with the use of the polynomial equations obtained, and an optimization diagram is presented. The minimum area shrinkage after washing and the least degradation of wool fibres are obtained with a Basolan DC concentration between 2.5 and 4.5% on the mass of wool and a pH value between 4 and 5.
引用
收藏
页码:49 / 56
页数:8
相关论文
共 17 条
[1]  
BLAKEY PR, 1969, J SOC DYERS COLOUR, V85, P107
[2]  
BROWN JC, 1972, REV PROG COLORATION, V3, P43
[3]   DYEING OF NYLON-66 WITH DISPERSE DYES - AN OPTIMIZATION STUDY [J].
CARPIGNANO, R ;
SAVARINO, P ;
BARNI, E ;
VISCARDI, G ;
BARACCO, A ;
CLEMENTI, S .
DYES AND PIGMENTS, 1989, 10 (01) :23-31
[4]   SHRINKPROOFING UNTREATED WOOL WITH HERCOSETT/UVITEX NFW-HYDROGEN PEROXIDE SYSTEMS - PHYSICOCHEMICAL PROPERTIES OF THESE SYSTEMS [J].
DELAMAZA, A ;
PARRA, JL ;
MANICH, AM ;
DECASTELLAR, MD .
TEXTILE RESEARCH JOURNAL, 1990, 60 (12) :709-713
[5]  
FRIEDRICH S, 1990, MELLIAND TEXTILBER, V71, P148
[6]  
HICKMAN WS, 1988, J SOC DYERS COLOUR, V104, P213
[7]  
MERTENS H, 1963, MELLIAND TEXTILBER, V44, P395
[8]  
SCHEFER W, 1978, TEXTILVEREDLUNG, V13, P55
[9]  
SOUREN I, 1984, J SOC DYERS COLOUR, V100, P378
[10]  
WURZ A, 1961, MELLIAND TEXTILBER, V42, P439