EXPERIENCE WITH THE MERRY-GO-ROUND TEST

被引:10
作者
GUBANSKI, SM [1 ]
机构
[1] WROCLAW TECH UNIV,INST ELECT ENGN FUNDAMENTALS,PL-50370 WROCLAW,POLAND
来源
IEEE TRANSACTIONS ON ELECTRICAL INSULATION | 1990年 / 25卷 / 02期
关键词
D O I
10.1109/14.52380
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Studies of the Merry-go-round test (MGR), using a newly-built apparatus, and their influence on the performance of different HV polymeric outdoor insulation housing materials are presented. In the test, the surface leakage currents, mass and wettability changes of the studied samples were monitored. The investigated materials were bisphenolic and cycloaliphatic epoxies, HTV and RTV silicone rubbers, and EPDM rubbers. Results show that the epoxies containing a silane-treated filler perform very well in the test. On the other hand, the silicone rubber performance, except for preservation of its hydrophobic properties, was comparable to the EPDM ones. This is contradictory to the material's field performance and indicates that there are still problems with interpretation of the MGR test results as well as their correlation to natural service experience. © 1990 IEEE
引用
收藏
页码:331 / 340
页数:10
相关论文
共 13 条