FACTORS AFFECTING STRESS-CORROSION CRACKING OF ZIRCALOY IN IODINE VAPOR

被引:85
作者
WOOD, JC [1 ]
机构
[1] ATOM ENERGY CANADA LTD,NUCL LABS,CHALK RIVER,ONTARIO,CANADA
关键词
D O I
10.1016/0022-3115(72)90178-X
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
引用
收藏
页码:105 / 122
页数:18
相关论文
共 17 条
[1]  
COX B, 1969, AECL3551 REP
[2]  
DIETER GE, 1961, MECHANICAL METALLURG, P405
[3]  
DRUCKER DC, 1963, AIME MET SOC C, V20
[4]  
FARMERY HK, 1956, J I MET, V84, P413
[5]   The production of pure metals from the titanium group through the thermic decomposition of iodine IV The occurrence of low zircon iodide in the production of ductile zircon [J].
Fast, JD .
ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE, 1938, 239 (02) :145-154
[6]   FRACTURE OF ZIRCONIUM ALLOYS IN IODINE VAPOUR [J].
GARLICK, A ;
WOLFENDEN, PD .
JOURNAL OF NUCLEAR MATERIALS, 1971, 41 (03) :274-+
[7]  
GARLICK A, 1971, M BRIT NUCLEAR ENERG
[8]  
GARLICK A, 1972, PRIVATE COMMUNICATIO
[9]  
HYATT MV, 1970, D624840 BOEING REP
[10]  
LORENZ RA, 1971, ORNL4635 USAEC REP