MECHANICAL STRENGTH INCREASE OF ABRADED SILICA GLASS BY HIGH-PRESSURE WATER-VAPOR TREATMENT

被引:25
作者
LI, H
TOMOZAWA, M
机构
[1] Materials Engineering Department, Rensselaer Polytechnic Institute, Troy
关键词
D O I
10.1016/0022-3093(94)90341-7
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The mechanical strength of abraded silica glass was increased by more than 200% by a saturated water vapor treatment at 250-degrees-C for 4 days. Fatigue resistance of the glass also improved with the treatment. The apparent flaw size estimated by optical microscopy remained unchanged. These features can be explained in terms of the crack tip blunting caused by dissolution and re-precipitation of silica glass assisted by capillary condensation of water near the crack tip, or by viscous flow of the glass containing water.
引用
收藏
页码:287 / 292
页数:6
相关论文
共 11 条
[1]  
BANDO Y, 1984, J AM CERAM SOC, V67, pC36
[2]   DYNAMIC FATIGUE OF GLASS [J].
CHARLES, RJ .
JOURNAL OF APPLIED PHYSICS, 1958, 29 (12) :1657-1662
[3]  
HAN WT, 1991, CERAMIC T, V20, P183
[4]   DYNAMIC FATIGUE OF TREATED HIGH-SILICA GLASS - EXPLANATION BY CRACK TIP BLUNTING [J].
HIRAO, K ;
TOMOZAWA, M .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1987, 70 (06) :377-382
[5]   CRACK BLUNTING OF HIGH-SILICA GLASS [J].
ITO, S ;
TOMOZAWA, M .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1982, 65 (08) :368-371
[6]   SHARP VS BLUNT CRACK HYPOTHESES IN THE STRENGTH OF GLASS - A CRITICAL-STUDY USING INDENTATION FLAWS [J].
LAWN, BR ;
JAKUS, K ;
GONZALEZ, AC .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1985, 68 (01) :25-34
[7]  
Marshall DB., 1985, STRENGTH INORGANIC G, P171
[8]  
MOORE DS, 1989, INTRO PRACTICE STAT, pCH8
[9]   INTERFACIAL LAYERS IN BRITTLE CRACKS [J].
ROACH, DH ;
LATHABAI, S ;
LAWN, BR .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1988, 71 (02) :97-105
[10]   RADIATION EFFECTS IN HYDROGEN-IMPREGNATED VITREOUS SILICA [J].
SHELBY, JE .
JOURNAL OF APPLIED PHYSICS, 1979, 50 (05) :3702-3707