DEACTIVATION OF HYDRODESULFURIZATION CATALYSTS UNDER COAL LIQUIDS .2. LOSS OF HYDROGENATION ACTIVITY DUE TO ADSORPTION OF METALLICS

被引:35
作者
KOVACH, SM
CASTLE, LJ
BENNETT, JV
SCHRODT, JT
机构
[1] UNIV KENTUCKY,DEPT CHEM ENGN,LEXINGTON,KY 40506
[2] ASHLAND OIL INC,ASHLAND,KY 41101
来源
INDUSTRIAL & ENGINEERING CHEMISTRY PRODUCT RESEARCH AND DEVELOPMENT | 1978年 / 17卷 / 01期
关键词
D O I
10.1021/i360065a017
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Minerals identified in coal were investigated as to their poisoning effect on the hydrogenation activity of several HDS catalysts under coal liquefaction conditions. Techniques of impregnation and exposure of catalysts to metal compounds were developed that allow the determination of rates of adsorption, poisoning, and loss of activity. The metals Na, K, Mg, Ca, P, Ti, Fe, and Si were shown to permanently poison catalysts at different rates. Deposition of carbonaceous mineral within the catalyst pores suppresses the adsorption of coal-liquid insoluble constituents. However, organometallics, such as those of titanium, are soluble in coal liquids, gain access to the surfaces, and are adsorbed in high concentrations. © 1978, American Chemical Society. All rights reserved.
引用
收藏
页码:62 / 67
页数:6
相关论文
共 5 条
  • [1] HOLLOWAY PH, 1976, SAND760644 ERDA REPT
  • [2] MORITZ KH, 1971, J CHEM ENG PROG, V67, P53
  • [3] DEACTIVATION OF HYDRODESULFURIZATION CATALYSTS UNDER COAL LIQUIDS .1. LOSS OF HYDROGENATION ACTIVITY DUE TO CARBONACEOUS DEPOSITS
    OCAMPO, A
    SCHRODT, JT
    KOVACH, SM
    [J]. INDUSTRIAL & ENGINEERING CHEMISTRY PRODUCT RESEARCH AND DEVELOPMENT, 1978, 17 (01): : 56 - 61
  • [4] CHEMISTRY AND ENGINEERING OF CATALYTIC HYDRODESULFURIZATION
    SCHUIT, GCA
    GATES, BC
    [J]. AICHE JOURNAL, 1973, 19 (03) : 417 - 438
  • [5] CATALYST AGING IN A PROCESS FOR LIQUEFACTION AND HYDRODESULFURIZATION OF COAL
    STANULONIS, JJ
    GATES, BC
    OLSON, JH
    [J]. AICHE JOURNAL, 1976, 22 (03) : 576 - 581