This study of internal hydrogen-induced crack growth in the iron-based superalloy IN903 shows that slow crack growth thresholds are significantly lower than fracture toughness values at the same precharged hydrogen concentrations. However, failure in all precharged samples occurred by slip band fracture which differed only in the extent of local surface plasticity. Quantitative fractography of these surface fracture features indicates that the crack tip hydrogen concentrations at threshold were higher than in fracture toughness samples. These higher concentrations are due to crack tip stress enhancement when sufficient time exists for hydrogen redistribution. In addition, continuum models based on mechanisms of failure demonstrate that the matrix carbides control crack growth susceptibility in slow crack growth and fracture toughness samples by establishing the characteristic distance that the crack tip stresses and strains must span to initiate fracture.
引用
收藏
页码:941 / 954
页数:14
相关论文
共 44 条
[31]   PLANE STRAIN DEFORMATION NEAR A CRACK TIP IN A POWER-LAW HARDENING MATERIAL [J].
RICE, JR ;
ROSENGREN, GF .
JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1968, 16 (01) :1-+
[32]   FURTHER CONSIDERATIONS ON INCONSISTENCY IN TOUGHNESS EVALUATION OF AISI 4340 STEEL AUSTENITIZED AT INCREASING TEMPERATURES [J].
RITCHIE, RO ;
HORN, RM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (03) :331-341
[33]   EVALUATION OF TOUGHNESS IN AISI 4340 ALLOY-STEEL AUSTENITIZED AT LOW AND HIGH-TEMPERATURES [J].
RITCHIE, RO ;
FRANCIS, B ;
SERVER, WL .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1976, 7 (06) :831-838
[34]   ON MACROSCOPIC AND MICROSCOPIC ANALYSES FOR CRACK INITIATION AND CRACK-GROWTH TOUGHNESS IN DUCTILE ALLOYS [J].
RITCHIE, RO ;
THOMPSON, AW .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1985, 16 (02) :233-248
[35]   HYDROGEN PERMEATION AND DIFFUSION IN INCONEL-718 AND INCOLOY-903 [J].
ROBERTSON, WM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1977, 8 (11) :1709-1712
[36]   REVIEW AND EXTENSION OF COMPLIANCE INFORMATION FOR COMMON CRACK GROWTH SPECIMENS [J].
SAXENA, A ;
HUDAK, SJ .
INTERNATIONAL JOURNAL OF FRACTURE, 1978, 14 (05) :453-468
[37]  
SCHULTE RL, 1981, HYDROGEN EFFECTS MET, P177
[38]  
SCHWALBE KH, 1977, T ASME H, V99, P186
[39]  
SINGH S, 1982, METALL T A, V13, P1979
[40]   STRUCTURE-PROPERTY-CONTINUUM SYNTHESIS OF DUCTILE FRACTURE IN INCONEL ALLOY 718 [J].
STOUT, MG ;
GERBERICH, WW .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (05) :649-658