OXIDATIVE BIODEGRADATION MECHANISMS OF BIAXIALLY STRAINED POLY(ETHERURETHANE UREA) ELASTOMERS

被引:108
作者
SCHUBERT, MA
WIGGINS, MJ
SCHAEFER, MP
HILTNER, A
ANDERSON, JM
机构
[1] CASE WESTERN RESERVE UNIV,DEPT MACROMOLEC SCI,CLEVELAND,OH 44106
[2] CASE WESTERN RESERVE UNIV,INST PATHOL,CLEVELAND,OH 44106
来源
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH | 1995年 / 29卷 / 03期
关键词
D O I
10.1002/jbm.820290309
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
As part of ongoing studies in polyurethane biostability and biodegradation, we have investigated an in vitro system to test strained poly(etherurethane urea) (PEUU). Recently, we utilized this system to reproduce in vivo stress cracking in strained Pellethane(R). In this study, strained PEUU was tested to determine whether it degrades through a common mechanism with Pellethane(R) and to further examine the steps involved in this degradation. Biaxially strained PEUU elastomers were treated with an alpha(2)-macroglobulin (alpha(2)-Mac) protein solution followed by an oxidative H2O2/CoCl2 treatment. Characterization of the strained PEUU specimens was performed with attenuated total reflectance-Fourier transform infrared spectroscopy, scanning electron microscopy (SEM), electron spectroscopy for chemical analysis, and contact angle analysis. The results from these characterization techniques provide conclusive evidence that biodegradation of PEUU and Pellethane(R) occurs through a common mechanism. Chemical changes to the PEUU include cleavage of the polyether soft segments and urethane linkages, leaving the hard segment domains unaffected. SEM analysis shows that this chain cleavage leads to the development of severe pitting and cracking of the PEUU surface. In addition, the in vitro degradation accurately reproduces the in vivo degradation chemically and physically. This result verifies that the primary species responsible for biodegradation of PEUUs, in vivo, are hydroxyl and/or hydroperoxide radicals. alpha(2)-Mac pretreatment increases the rate of degradation compared to direct treatment in H2O2/CoCl2. As the PEUU soft segment chains are cleaved, the degradation products are extracted into the treatment solution or environment. Finally, a new biodegradation mechanism of PEUUs is presented that involves crosslinking of the polyether soft segments. (C) 1995 John Wiley & Sons, Inc.
引用
收藏
页码:337 / 347
页数:11
相关论文
共 25 条
[1]  
Coury A J, 1988, J Biomater Appl, V3, P130, DOI 10.1177/088532828800300202
[2]  
Dillon J. G., 1989, INFRARED SPECTROSCOP
[3]  
GILDING DK, 1981, FUNDAMENTAL ASPECTS, pCH3
[4]   NORMAL VIBRATIONS OF POLYMER MOLECULES OF HELICAL CONFORMATION .6. POLYTETRAHYDROFURAN AND DEUTERATED POLYTETRAHYDROFURANS [J].
IMADA, K ;
TADOKORO, H ;
UMEHARA, A ;
MURAHASH.S .
JOURNAL OF CHEMICAL PHYSICS, 1965, 42 (08) :2807-&
[5]  
KAMBIC HE, 1986, CHEM ENG NEWS 0414, P31
[6]  
Lelah M. D., 1986, POLYURETHANES MED
[7]  
MARCH J, 1992, ADV ORGANIC CHEM REA, P378
[8]   INVIVO BIOCOMPATIBILITY STUDIES .1. THE CAGE IMPLANT SYSTEM AND A BIODEGRADABLE HYDROGEL [J].
MARCHANT, R ;
HILTNER, A ;
HAMLIN, C ;
RABINOVITCH, A ;
SLOBODKIN, R ;
ANDERSON, JM .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1983, 17 (02) :301-325
[9]   DEGRADATION OF MEDICAL-GRADE POLYURETHANE ELASTOMERS - THE EFFECT OF HYDROGEN-PEROXIDE INVITRO [J].
MEIJS, GF ;
MCCARTHY, SJ ;
RIZZARDO, E ;
CHEN, YC ;
CHATELIER, RC ;
BRANDWOOD, A ;
SCHINDHELM, K .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1993, 27 (03) :345-356
[10]  
PACKER JE, 1974, CHEM THIOL GROUP