共 17 条
[1]
Chow S. Z., 1969, Wood Science, V1, P215
[2]
Chow S. Z., 1969, Forest Products Journal, V19, P21
[3]
HANCOCK WV, 1964, THESIS U BRITISH COL, P176
[4]
HEMINGWAY RW, 1967, THESIS U MICHIGAN, P157
[5]
THE DEGRADATION OF CELLULOSE IN AIR AT 250-DEGREES-C AS SHOWN BY INFRARED SPECTROSCOPIC EXAMINATION
[J].
JOURNAL OF POLYMER SCIENCE,
1958, 28 (118)
:645-648
[6]
JURECIC A, 1966, TAPPI, V49, P306
[7]
INFRARED SPECTRA OF CRYSTALLINE POLYSACCHARIDES .1. HYDROGEN BONDS IN NATIVE CELLULOSES
[J].
JOURNAL OF POLYMER SCIENCE,
1959, 37 (132)
:385-395
[8]
MAJOR WD, 1958, TAPPI, V41, P530
[9]
Marchessault R.H., 1962, PURE APPL CHEM, V5, P107, DOI DOI 10.1351/PAC196205010107
[10]
Northcott P. C., 1957, Forest Products Journal, V7, P10