Impact strength of denture polymethyl methacrylate reinforced with continuous glass fibers or metal wire

被引:65
作者
Vallittu, PK [1 ]
Vojtkova, H [1 ]
Lassila, VP [1 ]
机构
[1] DENT AS, DIV RES & DEV, PRAGUE, CZECH REPUBLIC
关键词
acrylic resins; dentures; reinforcement;
D O I
10.3109/00016359509006007
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The impact strength of heat-cured acrylic resin test specimens that had been reinforced in various ways was compared in this study. Ten rectangular test specimens were fabricated for each test group. The strengtheners included 1.0-mm-diameter steel wire and continuous E-glass fibers. Both notched and unnotched test specimens were tested in a Charpy-type impact rest. In a further analysis the concentration of glass fibers in the test specimens was determined and plotted against the impact strength of the test specimens. The results showed that; compared with the unreinforced specimens, both types of reinforcement increased the impact strength of the test specimens considerably (P < 0.001). There was no clear difference between the mean impact strength value of the test specimens reinforced with metal wire and that of the specimens reinforced with glass fiber. The correlation coefficient between the fiber concentration of the test specimens and their impact strength was 0.818 (P < 0.005). Specimens with fiber concentrations greater than 25 wt% yielded to the higher impact strength more readily than those with metal wire reinforcement did.
引用
收藏
页码:392 / 396
页数:5
相关论文
共 35 条
[1]  
AIRASMAA I, 1984, LUJITEMUOVITEKNIIKKA, P246
[2]  
Berrong J M, 1990, Int J Prosthodont, V3, P391
[3]   WIRE REINFORCEMENT OF ACRYLIC RESIN PROSTHESES [J].
CARROLL, CE ;
VONFRAUNHOFER, JA .
JOURNAL OF PROSTHETIC DENTISTRY, 1984, 52 (05) :639-641
[4]   THE EFFECT OF CARBON-FIBER ORIENTATION ON THE FATIGUE RESISTANCE AND BENDING PROPERTIES OF 2 DENTURE RESINS [J].
DEBOER, J ;
VERMILYEA, SG ;
BRADY, RE .
JOURNAL OF PROSTHETIC DENTISTRY, 1984, 51 (01) :119-121
[5]   THE TRANSVERSE STRENGTHS OF 3 DENTURE BASE RESINS REINFORCED WITH POLYETHYLENE FIBERS [J].
DIXON, DL ;
BREEDING, LC .
JOURNAL OF PROSTHETIC DENTISTRY, 1992, 67 (03) :417-419
[6]  
DIXON DL, 1981, J PROSTHET DENT, V64, P4178
[7]   CARBON GRAPHITE FIBER REINFORCED POLY(METHYL METHACRYLATE) - PROPERTIES UNDER DRY AND WET CONDITIONS [J].
EKSTRAND, K ;
RUYTER, IE ;
WELLENDORF, H .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1987, 21 (09) :1065-1080
[8]   ACOUSTIC RELAXATION AND INFRARED SPECTROSCOPIC MEASUREMENTS OF PLASTICIZATION OF POLY(METHYL METHACRYLATE) BY WATER [J].
GILBERT, AS ;
PETHRICK, RA ;
PHILLIPS, DW .
JOURNAL OF APPLIED POLYMER SCIENCE, 1977, 21 (02) :319-330
[9]   THE USE OF CONTINUOUS FIBER REINFORCEMENT IN DENTISTRY [J].
GOLDBERG, AJ ;
BURSTONE, CJ .
DENTAL MATERIALS, 1992, 8 (03) :197-202
[10]   REINFORCEMENT OF POLY(METHYL METHACRYLATE) WITH ULTRA-HIGH-MODULUS POLYETHYLENE FIBER [J].
GUTTERIDGE, DL .
JOURNAL OF DENTISTRY, 1992, 20 (01) :50-54