THE INFLUENCE OF OPERATING AND COKE-RELATED VARIABLES ON THE REGENERATION OF FIXED-BEDS OF CATALYST

被引:17
作者
BYRNE, A [1 ]
HUGHES, R [1 ]
SANTAMARIA, J [1 ]
机构
[1] UNIV SALFORD,DEPT CHEM & GAS ENGN,SALFORD M5 4WT,LANCS,ENGLAND
关键词
D O I
10.1016/0009-2509(89)85154-1
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
引用
收藏
页码:2197 / 2206
页数:10
相关论文
共 21 条
[1]   SIMPLE METHOD FOR APPROXIMATING ACTIVITY PROFILES IN A DEACTIVATING ADIABATIC REACTOR [J].
BRITOALAYON, A ;
HUGHES, R ;
KAM, EKT .
INDUSTRIAL & ENGINEERING CHEMISTRY FUNDAMENTALS, 1981, 20 (04) :399-403
[2]   THE INFLUENCE OF INITIAL COKE PROFILE AND HYDROGEN CONTENT OF COKE ON THE REGENERATION OF FIXED-BEDS OF CATALYST [J].
BYRNE, A ;
HUGHES, R ;
SANTAMARIARAMIRO, J .
CHEMICAL ENGINEERING SCIENCE, 1985, 40 (08) :1507-1516
[3]  
BYRNE A, 1986, J CATAL, V96, P146
[4]   COKE FORMATION ON SILICA-ALUMINA CRACKING CATALYSTS [J].
EBERLY, PE ;
KIMBERLI.CN ;
MILLER, WH ;
DRUSHEL, HV .
INDUSTRIAL & ENGINEERING CHEMISTRY PROCESS DESIGN AND DEVELOPMENT, 1966, 5 (02) :193-&
[5]   NON-STEADY STATE BEHAVIOUR OF FIXED BED CATALYTIC REACTORS DUE TO CATALYST FOULING [J].
FROMENT, GF ;
BISCHOFF, KB .
CHEMICAL ENGINEERING SCIENCE, 1961, 16 (3-4) :189-201
[6]   KINETIC DATA AND PRODUCT DISTRIBUTIONS FROM FIXED BED CATALYTIC REACTORS SUBJECT TO CATALYST FOULING [J].
FROMENT, GF ;
BISCHOFF, KB .
CHEMICAL ENGINEERING SCIENCE, 1962, 17 (02) :105-&
[7]   ON THE NATURE OF THE CARBON DEPOSIT OF CRACKING CATALYSTS [J].
HALDEMAN, RG ;
BOTTY, MC .
JOURNAL OF PHYSICAL CHEMISTRY, 1959, 63 (04) :489-496
[8]  
HANO T, 1976, J CHEM ENG JAPAN, V9, P209
[9]  
HUGHES R, 1970, J APPL CHEM BIOTECHN, V21, P35
[10]   TEMPERATURE PROFILES IN PACKED BEDS OF CATALYST DURING REGENERATION [J].
JOHNSON, BM ;
FROMENT, GF ;
WATSON, CC .
CHEMICAL ENGINEERING SCIENCE, 1962, 17 (11) :835-&