MECHANICAL-PROPERTIES OF MOSTLY-CRYSTALLINE, RAPID-QUENCHED PD-SI-SB

被引:2
作者
MARCUS, MA [1 ]
机构
[1] HARVARD UNIV,CAMBRIDGE,MA 02138
来源
ACTA METALLURGICA | 1979年 / 27卷 / 05期
关键词
D O I
10.1016/0001-6160(79)90124-X
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The mechanical properties of some rapid-quenched, partly-amorphous (as-prepared) PdSiSb alloys have been studied. These alloys showed tensile strengths (fracture force/fracture surface area) of 58-232 kg/mm2, depending on their amorphous fraction (0-6%). The alloy's high strengths are due to an unusual microstructure, which consists of fine ( < 1 μm) dendrites of a ductile, supersaturated solution of Si and Sb in f.c.c. Pd, embedded in an amorphous matrix. The role of the glassy matrix in the fracture process is discussed. © 1979.
引用
收藏
页码:893 / 902
页数:10
相关论文
共 10 条
[1]   MECHANISM OF FRACTURE IN GLASSY MATERIALS CAPABLE OF SOME INELASTIC DEFORMATION [J].
ARGON, AS ;
SALAMA, M .
MATERIALS SCIENCE AND ENGINEERING, 1976, 23 (2-3) :219-230
[2]  
CHOU P, 1975, ACTA METALL, V23, P609
[3]  
DAVIS L, 1978, STRENGTH DUCTILITY T
[4]  
MARCUS M, UNPUBLISHED
[5]   STRUCTURAL STABILITY AND MECHANICAL-PROPERTIES OF AMORPHOUS METALS [J].
MASUMOTO, T ;
MADDIN, R .
MATERIALS SCIENCE AND ENGINEERING, 1975, 19 (01) :1-24
[6]  
MEGUSAR J, 1976, RAPIDLY QUENCHED MET
[7]  
SAFFMAN PG, 1958, P R SOC LOND A, V245, P322
[8]   MICROSCOPIC MECHANISM FOR STEADY-STATE INHOMOGENEOUS FLOW IN METALLIC GLASSES [J].
SPAEPEN, F .
ACTA METALLURGICA, 1977, 25 (04) :407-415
[9]   MECHANISM FOR FLOW AND FRACTURE OF METALLIC GLASSES [J].
SPAEPEN, F ;
TURNBULL, D .
SCRIPTA METALLURGICA, 1974, 8 (05) :563-568
[10]  
1961, METALS HDB, V1