BEHAVIOR OF MORTAR AND CONCRETE AT EXTREMELY LOW-TEMPERATURES

被引:64
作者
ROSTASY, FS
SCHNEIDER, U
WIEDEMANN, G
机构
[1] Institut für Baustoffe, Massivbau und Brandschutz Technische Universität Braunschweig
关键词
D O I
10.1016/0008-8846(79)90129-7
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
The behaviour of hydrated cement paste, mortar and concrete specimens (age ∼ 110 days) was investigated at low temperatures and after cyclic temperature-time histories. The relative changes of thermal strains, compressive and tensile splitting strength as well as the alteration of pore structure were studied. The strength in the frozen state increases with decreasing temperature and rising moisture content. If the frozen water-saturated mortar or concrete is reheated to room temperature a loss of strength is registered. The loss of strength increases with the number of temperature cycles. Storing the specimens at rel. hum. below 85% no losses were registered and no irreversible expansion occured. Water-saturated mortar showed after only 12 cycles an irreversible positive strain of 2,7%, indicating internal damage which was also proved by mercury porosimetry. Thus, the moisture content seems to be one of the decisive factors affecting the sensitivity of mortar and concrete subjected to extremely low temperatures. © 1979.
引用
收藏
页码:365 / 376
页数:12
相关论文
共 10 条
[1]  
Wischers, Dahms, Das Verhalten des Betons bei sehr niedrigen Temperaturen, (1970)
[2]  
Saemann, Washa, Variation of mortar and concrete properties with temperature, Proc. Amer. Concr. Inst., 54, (1957)
[3]  
Monfore, Lentz, Physical properties of concrete at very low temperatures, P.C.A. Research Dept. Bulletin No. 145, (1962)
[4]  
Lentz, Monfore, Thermal conductivity of concrete at very low temperatures, Journal of the P.C.A. Research and Development Laboratories, (1965)
[5]  
Lentz, Monfore, Thermal conductivities of portland cement paste, aggregate, and concrete down to very low temperatures, Journal of the P.C.A. Research and Development Laboratories, (1966)
[6]  
Radjy, A thermodynamic study of the system hardened cement paste and water and its dynamic mechanical response as a function of temperature, Dissertation, (1968)
[7]  
Moskvin, Kaptien, Antonow, Einfluβ von Temperaturen unterhalb des Frostbereiches auf die Festigkeit und die elestoplastischen Eigenschaften von Beton, Beton i zelezobeton, 13, (1967)
[8]  
Tognon, Behaviour of mortars and concretes in the temperature range from +20°C to −196°C, Supplementary Paper III-24, (1968)
[9]  
Marechal, Thermal conductivity and thermal expansion coefficients of concrete as a function of temperature and humidity, ACI-Int. Seminar on CNR, (1970)
[10]  
Radjy, Richards, Internal friction and dynamic modulus transistions in hardened cement paste at low temperatures, Matériaux et Constructions, 7, (1969)