NEW MECHANISM FOR LENGTHENING THE LIFETIME OF HYDROGENATION CATALYSTS

被引:19
作者
SCHLAPBACH, L
SEILER, A
STUCKI, F
机构
[1] Laboratorium für Festkörperphysik ETH Zürich
关键词
D O I
10.1016/0025-5408(79)90138-7
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Intermetallic compounds with d-transition metals have been used as catalysts. XPS and AES studies and the magnetic properties of LaNi5 and FeTi show that surface segregation occurs and that superparamagnetic Ni and Fe precipitates are formed at the surface, catalyzing the dissociation of molecular hydrogen. The catalytic activity of many intermetallic compounds can be explained by surface segregation and the formation of d-transition metal precipitates. Contaminants often drive the segregation, hereby prolonging the lifetime of the catalyst. We predict that FeTi can replace Fe-catalysts being more resistant to contaminants. © 1979.
引用
收藏
页码:785 / 790
页数:6
相关论文
共 20 条
[1]   MISCHMETAL-NICKEL ALLOYS AS METHANATION CATALYSTS [J].
ATKINSON, GB ;
NICKS, LJ .
JOURNAL OF CATALYSIS, 1977, 46 (03) :417-419
[2]   PREDICTION OF SEGREGATION TO ALLOY SURFACES FROM BULK PHASE-DIAGRAMS [J].
BURTON, JJ ;
MACHLIN, ES .
PHYSICAL REVIEW LETTERS, 1976, 37 (21) :1433-1436
[3]   CONVERSION OF ETHYLENE TO ACETYLENE ON NI(111) [J].
DEMUTH, JE .
SURFACE SCIENCE, 1978, 76 (02) :L603-L608
[4]  
FISCHER P, 1977, HELV PHYS ACTA, V50, P421
[5]  
FISCHER P, 1978, MAT RES B, V13, P1031
[6]  
KUIJPERS FA, 1971, J PHYS COLLOQUES, V32, pC1
[7]   CATALYSIS OF CARBON-MONOXIDE AND CARBON-DIOXIDE METHANATION BY CEAL2, CECO2, CENI2, CO, AND NI [J].
LUENGO, CA ;
CABRERA, AL ;
MACKAY, HB ;
MAPLE, MB .
JOURNAL OF CATALYSIS, 1977, 47 (01) :1-10
[8]  
MIEDEMA AR, 1978, Z METALLKD, V69, P455
[9]   SURFACE COMPOSITION OF BINARY-SYSTEMS - PREDICTION OF SURFACE PHASE-DIAGRAMS OF SOLID-SOLUTIONS [J].
OVERBURY, SH ;
BERTRAND, PA ;
SOMORJAI, GA .
CHEMICAL REVIEWS, 1975, 75 (05) :547-560
[10]  
POUNTNEY JM, 1978, 37 I PHYS C SER, P85