EFFECTS OF MICROSTRUCTURAL INSTABILITY ON THE CREEP-BEHAVIOR OF SI-C-O (NICALON) FIBERS IN ARGON

被引:32
作者
JIA, NY [1 ]
BODET, R [1 ]
TRESSLER, RE [1 ]
机构
[1] PENN STATE UNIV,CTR ADV MAT,UNIV PK,PA 16802
关键词
D O I
10.1111/j.1151-2916.1993.tb06608.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Tensile creep tests of single Si-C-0 fibers (Nicalon, Nippon Carbon Co., Tokyo, Japan) were conducted in argon at 1300-degrees-C and 300 to 700 MPa. Fibers exhibited only primary creep, where the creep strain epsilon and creep time t could be empirically fitted by epsilon = (1/beta) In (1 + betaepsilon0t). The fiber deformation was described by a rheological model for the viscous flow of a concentrated suspension. Under the test conditions, the microstructure of Nicalon was unstable, resulting in weight loss and SiC grain growth. This instability was attributed to the decomposition of the amorphous SiC(x)O(x) phase in the fiber, forming SiC and CO as products. As a result, the viscosity of the fiber increased because of an increase in the SiC volume fraction. The continuous increase in viscosity caused a continuously decreasing creep rate, which made steady-state creep impossible under these conditions. Because of the instability in the microstructure, the chemical environment was found to have a profound influence on the mechanical properties of Nicalon at elevated temperatures.
引用
收藏
页码:3051 / 3060
页数:10
相关论文
共 54 条
[1]   CREEP-BEHAVIOR AND MICROSTRUCTURAL CHARACTERIZATION OF A CERAMIC MATRIX COMPOSITE [J].
ABBE, F ;
VICENS, J ;
CHERMANT, JL .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1989, 8 (09) :1026-1028
[2]   SILICON-CARBIDE FIBERS AND THEIR POTENTIAL FOR USE IN COMPOSITE-MATERIALS .1. [J].
ANDERSSON, CH ;
WARREN, R .
COMPOSITES, 1984, 15 (01) :16-24
[4]   EFFECT OF BROWNIAN-MOTION ON BULK STRESS IN A SUSPENSION OF SPHERICAL-PARTICLES [J].
BATCHELOR, GK .
JOURNAL OF FLUID MECHANICS, 1977, 83 (NOV) :97-117
[5]   EFFECT OF THERMOCHEMICAL TREATMENTS ON THE STRENGTH AND MICROSTRUCTURE OF SIC FIBERS [J].
BENDER, BA ;
WALLACE, JS ;
SCHRODT, DJ .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (04) :970-976
[6]  
Benson P.M, 1988, CERAM ENG SCI P, V9, P663
[7]   EFFECT OF CARBON-MONOXIDE PARTIAL-PRESSURE ON THE HIGH-TEMPERATURE DECOMPOSITION OF NICALON FIBER [J].
BIBBO, GS ;
BENSON, PM ;
PANTANO, CG .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (18) :5075-5080
[8]  
BODET R, 1991, THESIS PENNSYLVANIA
[9]   COMPOSITION MICROSTRUCTURE PROPERTY RELATIONSHIPS IN CERAMIC MONOFILAMENTS RESULTING FROM THE PYROLYSIS OF A POLYCARBOSILANE PRECURSOR AT 800 TO 1400-DEGREES-C [J].
BOUILLON, E ;
MOCAER, D ;
VILLENEUVE, JF ;
PAILLER, R ;
NASLAIN, R ;
MONTHIOUX, M ;
OBERLIN, A ;
GUIMON, C ;
PFISTER, G .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (06) :1517-1530
[10]  
BRENNAN JJ, 1986, TAILORING MULTIPHASE, V20, P549