Passivity breakdown experiments have been performed on a duplex stainless steel in 0. 5N HCI, H//2O/methanol solutions as a function of delta -ferrite content and water/methanol ratios. The pitting resistance in strongly passivating (aqueous) solutions is primarily a function of the composition of delta / gamma interface, relatively independent of the interfacial area or of the ferrite content higher than 1 Vol%. The integrity of the passive film is thought to be associated with segregation of sulfur to the delta / gamma interface. Pits initiate in duplex alloy at the delta /65 phase boundaries, in the single phase alloy at sulfide inclusions.
引用
收藏
页码:63 / 68
页数:6
相关论文
共 37 条
[1]  
Andersson B. R. T., 1975, SCAND J METALL, V4, P85
[2]  
BOHNI H, INTERNAL REPORTS ETH
[3]  
BRAUNS E, 1961, WERKST KORROS, V12, P73
[4]  
BUEHLER HE, 1964, WERKST KORROSION, V15, P909
[5]  
DEGERBECK J, 1978, WERKST KORROS, V29, P179
[6]  
DEGERBECK J, 1974, WERKST KORROS, V25, P172
[8]   MECHANISM OF INTERGRANULAR CORROSION AND PITTING CORROSION OF AUSTENITIC AND DUPLEX 308 STAINLESS-STEEL [J].
DEVINE, TM .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1979, 126 (03) :374-385
[9]  
Eklund G., 1972, SCAND J METALL, V1, P331
[10]   INITIATION OF CREVICE CORROSION ON STAINLESS-STEEL [J].
EKLUND, GS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (02) :170-173