THERMAL EFFECTS ON THE MECHANICAL-PROPERTIES OF SIC FIBER REINFORCED REACTION-BONDED SILICON-NITRIDE MATRIX COMPOSITES

被引:12
作者
BHATT, RT [1 ]
PHILLIPS, RE [1 ]
机构
[1] SVERDRUP TECHNOL INC,NASA,LEWIS RES CTR GRP,CLEVELAND,OH 44135
关键词
D O I
10.1007/BF00587704
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The elevated temperature four-point flexural strength and the room-temperature tensile and flexural strength properties after thermal shock were measured for ceramic composites consisting of 30 vol% uniaxially aligned 142 μm diameter SiC fibres in a reaction-bonded Si3N4 matrix. The elevated temperature strengths were measured after 15 min exposure in air at temperatures upto 1400 ° C. The thermal shock treatment was accomplished by heating the composite in air for 15 min at temperatures up to 1200 ° C and then quenching in water at 25 ° C. The results indicate no significant loss in strength properties either at temperature or after thermal shock when compared with the strength data for composites in the as-fabricated condition. © 1990 Chapman and Hall Ltd.
引用
收藏
页码:3401 / 3407
页数:7
相关论文
共 6 条
[1]  
Bhatt R. T., 1986, Tailoring Multiphase and Composite Ceramics. Proceedings of the Twenty-First University Conference on Ceramic Science, P675
[2]  
BHATT RN, IN PRESS
[3]  
BHATT RT, 1986, METAL CERAMIC MATRIX, P277
[4]  
LARSEN DC, 1984, IITRIM0611520 ILL I
[5]  
LARSEN DC, 1985, CERAMIC MATERIALS AD
[6]  
LUCEK JW, 1985, METAL MATRIX CARBON, P27