摘要
Beta-Si3N4 powder made by the imide-decomposition method was gas-pressure sintered at 1800 degrees C for 4h in 1 MPa N-2 gas. This material had a microstructure of ''in-situ composite'' and excellent mechanical properties (strength : 780 MPa, fracture toughness : 7.5 MPa . m(1/2)), whereas beta-Si3N4 powder made by the silicon nitridation method required sintering temperatures higher than 1900 degrees C to attain similar microstructure and mechanical properties. beta-Si3N4 powder by the imide-decomposition method had excellent properties for grain growth at low temperatures.
引用
收藏
页码:977 / 978
页数:2
相关论文
共 3 条
[1]  
HIROSAKI N, 1993, J AM CERAM SOC, V76, P892
[2]  
Knoch H., 1978, Berichte der Deutschen Keramischen Gesellschaft, V55, P242
[3]   RELATION BETWEEN STRENGTH, FRACTURE ENERGY, AND MICROSTRUCTURE OF HOT-PRESSED SI3N4 [J].
LANGE, FF .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1973, 56 (10) :518-522