OXIDATION BEHAVIOR OF TI3AL ALLOYED WITH NIOBIUM AND SILICON

被引:21
作者
QIU, GH
WU, JS
ZHANG, LT
机构
[1] Department of Materials Science Shanghai Jiao Tong University Shanghai
来源
SCRIPTA METALLURGICA ET MATERIALIA | 1995年 / 33卷 / 02期
关键词
D O I
10.1016/0956-716X(95)00150-T
中图分类号
T [工业技术];
学科分类号
08 [工学];
摘要
[No abstract available]
引用
收藏
页码:213 / 217
页数:5
相关论文
共 11 条
[1]
ESSOUNI M, 1991, P INT S INTERMETALLI, P525
[2]
SYNTHESIS, PROPERTIES AND APPLICATIONS OF TITANIUM ALUMINIDES [J].
FROES, FH ;
SURYANARAYANA, C ;
ELIEZER, D .
JOURNAL OF MATERIALS SCIENCE, 1992, 27 (19) :5113-5140
[3]
COMPOSITE TIAL3-TIN COATINGS ON TITANIUM [J].
KABBAJ, M ;
GALERIE, A ;
CAILLET, M .
JOURNAL OF THE LESS-COMMON METALS, 1985, 108 (01) :1-21
[4]
Kim Y.W., 1990, HIGH TEMPERATURE ALU, P485
[5]
THE DEFORMATION AND FRACTURE OF TI3AL AT ELEVATED-TEMPERATURES [J].
LIPSITT, HA ;
SHECHTMAN, D ;
SCHAFRIK, RE .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1980, 11 (08) :1369-1375
[6]
EFFECT OF SILICON AND NIOBIUM ON OXIDATION RESISTANCE OF TIAL INTERMETALLICS [J].
MAKI, K ;
SHIODA, M ;
SAYASHI, M ;
SHIMIZU, T ;
ISOBE, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 153 (1-2) :591-596
[7]
QIU GH, 1994, FAL MRS M BOST
[8]
HIGH-TEMPERATURE OXIDATION RESISTANCE OF TIAL IMPROVED BY IBED SI3N4 COATING [J].
TANIGUCHI, S ;
SHIBATA, T ;
YAMADA, T ;
LIU, XH ;
ZOU, SC .
ISIJ INTERNATIONAL, 1993, 33 (08) :869-876
[9]
WALLACE TA, 1992, OXID MET, V137, P111
[10]
THE BETA-TI(AL,SI)+TI5(SI,AL)3 EUTECTIC REACTION IN THE TI-AL-SI TERNARY-SYSTEM [J].
WU, JS ;
QIU, GH ;
ZHANG, LT .
SCRIPTA METALLURGICA ET MATERIALIA, 1994, 30 (02) :213-218