DAMAGE CHARACTERIZATION OF A 2D SIC-SIC COMPOSITE-MATERIAL

被引:5
作者
DESPIERRES, T
HABTI, MD
GOMINA, M
机构
[1] LERMAT, ISMRA, URA CNRS No. 1317, 14050 Caen Cedex
关键词
D O I
10.1016/0955-2219(93)90106-2
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 [材料科学与工程]; 080502 [材料学];
摘要
The damage characterization of a type of 2D SiC-SiC composite material made of Nicalon SiC fibres, a pyrocarbon interphase and a beta-SiC matrix is conducted using uniaxial tensile tests. Damage is evaluated by the variations of the Young's modulus and the total number of cracks (either in the total volume of the specimen or only between the fibres inside the bundles) as functions of the applied strain, from the end of the linear behaviour to failure. It is shown that the Aveston, Cooper and Kelly model commonly used for the interfacial shear stress estimation is not applicable to this material.
引用
收藏
页码:309 / 314
页数:6
相关论文
共 12 条
[1]
THEORY OF MULTIPLE FRACTURE OF FIBROUS COMPOSITES [J].
AVESTON, J ;
KELLY, A .
JOURNAL OF MATERIALS SCIENCE, 1973, 8 (03) :352-362
[2]
Aveston J, 1971, PROPERTIES FIBER COM, P15
[3]
COMPOSITION MICROSTRUCTURE PROPERTY RELATIONSHIPS IN CERAMIC MONOFILAMENTS RESULTING FROM THE PYROLYSIS OF A POLYCARBOSILANE PRECURSOR AT 800 TO 1400-DEGREES-C [J].
BOUILLON, E ;
MOCAER, D ;
VILLENEUVE, JF ;
PAILLER, R ;
NASLAIN, R ;
MONTHIOUX, M ;
OBERLIN, A ;
GUIMON, C ;
PFISTER, G .
JOURNAL OF MATERIALS SCIENCE, 1991, 26 (06) :1517-1530
[4]
STRUCTURAL MODIFICATIONS OF A SIC-SIC MATERIAL EXPOSED TO HIGH-TEMPERATURES IN AIR [J].
FOURVEL, P ;
SYLVESTRINI, P ;
ROUILLON, MH ;
VICENS, J ;
GOMINA, M .
JOURNAL OF MATERIALS SCIENCE, 1990, 25 (12) :5163-5165
[5]
GOMINA M, 1989, 1ST P EUR CER SOC C, V3, P366
[6]
JOSTE B, 1986, OBSERVATIONS MET MAT
[7]
Lowden R.A., 1988, CERAMIC ENG SCI P, V9, P705
[8]
LOWDEN RA, 1987, ORNLTM10667 REP
[9]
MADIGOU V, 1991, MICROSC MICROANAL MI, V2, P47
[10]
MANIETTE Y, 1988, THESIS U PAU PAYS AD