INFRARED STUDY OF THE FORMATION AND STABILITY OF LA2O2CO3 DURING THE OXIDATIVE COUPLING OF METHANE ON LA2O3

被引:116
作者
LEVAN, T
CHE, M
TATIBOUET, JM
KERMAREC, M
机构
[1] Laoratoire de Réactivité de Surface et Structure, URA 1106 CNRS, Université P. et M. Curie, 75252 Paris 05
关键词
D O I
10.1006/jcat.1993.1185
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The formation and stability of La2O2CO2 under CO2/He and the CH4/O2/He reaction mixture were investigated by infrared spectroscopy in the 650-750°C range. La2O2CO3 is not stable under flowing He at 650°C. Bulk La2O2CO3 is formed during the oxidative coupling of CH4 at 650°C, although thermodynamic considerations predict that it cannot be generated from the gaseous CO2 produced by the catalytic reaction. On this basis, it is suggested that the dioxymonocarbonate is formed via the surface deep oxidation of CH4 and/or the reaction products. FTIR spectroscopy indicates that 15% of the starting catalyst La2O3 is transformed into La2O2CO3 by the catalytic reaction at 650°C. © 1993 Academic Press, Inc.
引用
收藏
页码:18 / 26
页数:9
相关论文
共 33 条
  • [1] LANTHANIDE OXIDES - PREPARATION AND AGING
    ALVERO, R
    ODRIOZOLA, JA
    TRILLO, JM
    BERNAL, S
    [J]. JOURNAL OF THE CHEMICAL SOCIETY-DALTON TRANSACTIONS, 1984, (01): : 87 - &
  • [2] OXIDATIVE DEHYDROGENATION OF ETHANE OVER LANTHANA - ACTUAL NATURE OF THE ACTIVE PHASE
    BERNAL, S
    MARTIN, GA
    MORAL, P
    PERRICHON, V
    [J]. CATALYSIS LETTERS, 1990, 6 (02) : 231 - 238
  • [3] BEHAVIOR OF RARE-EARTH SESQUIOXIDES EXPOSED TO ATMOSPHERIC CARBON-DIOXIDE AND WATER
    BERNAL, S
    BOTANA, FJ
    GARCIA, R
    RODRIGUEZIZQUIERDO, JM
    [J]. REACTIVITY OF SOLIDS, 1987, 4 (1-2): : 23 - 40
  • [4] STUDY OF SOME ASPECTS OF THE REACTIVITY OF LA2O3 WITH CO2 AND H2O
    BERNAL, S
    DIAZ, JA
    GARCIA, R
    RODRIGUEZIZQUIERDO, JM
    [J]. JOURNAL OF MATERIALS SCIENCE, 1985, 20 (02) : 537 - 541
  • [5] CAMERON C, 1987, Patent No. 8711183
  • [6] CAMERON C, 1987, Patent No. 8716614
  • [7] CAMERON C, 1990, Patent No. 4929787
  • [8] CARO P, 1970, 1969 P C EL TERR RAR, V1, P285
  • [9] CARO PE, 1968, J LESS-COMMON MET, V16, P376
  • [10] KINETICS OF THE OXIDATIVE COUPLING OF METHANE OVER 1 WT-PERCENT SR/LA2O3
    DEBOY, JM
    HICKS, RF
    [J]. JOURNAL OF CATALYSIS, 1988, 113 (02) : 517 - 524