THE CATHODIC POLARIZATION OF ALUMINUM COVERED WITH ANODIC OXIDE-FILMS IN A NEUTRAL BORATE SOLUTION .2. FILM BREAKDOWN AND PIT FORMATION

被引:29
作者
TAKAHASHI, H
FUJIWARA, K
SEO, M
机构
[1] Faculty of Engineering, Hokkaido University, Kita-ku, Sapporo, 060
关键词
D O I
10.1016/0010-938X(94)90074-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Porous and barrier type oxide films were formed anodically on pure aluminum and dissolved chemically. The specimens were then cathodically polarized by the potential sweep method in a neutral borate solution. It was found that the cathodic current starts to increase at about -2 to -3 V(Ag/AgCl) and that at more negative potentials increases almost linearly, accompanied by hydrogen evolution. The cathodic polarization curve shifts in the anodic direction with decreasing film formation potential and increasing chemical dissolution time. During cathodic polarization, cubic-shape pits are formed by local corrosion of the metal substrate. The number of pits formed by cathodic polarization is larger for porous than for barrier type oxide films, while the pit number is independent of the film formation potential, it increases considerably with increasing chemical dissolution time. The ratio of the local corrosion rate to the electrochemical reaction rate during cathodic polarization is about 0.03 on specimens without chemical dissolution, and about 0.10 with chemical dissolution. The effect of film structure on the pit formation during cathodic polarization is discussed in terms of imperfections in the oxide.
引用
收藏
页码:689 / &
相关论文
共 8 条
[1]   ABNORMAL YIELDS OF HYDROGEN AND THE MECHANISM OF ITS EVOLUTION DURING CATHODIC POLARIZATION OF ALUMINUM [J].
DESPIC, AR ;
RADOSEVIC, J ;
DABIC, P ;
KLISKIC, M .
ELECTROCHIMICA ACTA, 1990, 35 (11-12) :1743-1746
[2]  
Ebihara K., 1983, J MET FINISH SOC JPN, V34, P548, DOI DOI 10.4139/SFJ1950.34.548
[3]   CATHODIC POLARIZATION OF COMMERCIALLY PURE ALUMINUM [J].
NISANCIOGLU, K ;
HOLTAN, H .
CORROSION SCIENCE, 1979, 19 (08) :537-552
[4]   PROCESSES ON ALUMINUM ON THE NEGATIVE SIDE OF THE OPEN-CIRCUIT POTENTIAL [J].
RADOSEVIC, J ;
KLISKIC, M ;
DABIC, P ;
STEVANOVIC, R ;
DESPIC, A .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1990, 277 (1-2) :105-119
[5]   ELECTROCHEMICAL BEHAVIOR AND STRUCTURE OF ANODIC OXIDE-FILMS FORMED ON ALUMINUM IN A NEUTRAL BORATE SOLUTION [J].
TAKAHASHI, H ;
NAGAYAMA, M .
ELECTROCHIMICA ACTA, 1978, 23 (03) :279-286
[6]   DETERMINATION OF POROSITY OF ANODIC OXIDE-FILMS ON ALUMINUM BY PORE-FILLING METHOD [J].
TAKAHASHI, H ;
NAGAYAMA, M .
CORROSION SCIENCE, 1978, 18 (10) :911-&
[7]   THE CATHODIC POLARIZATION OF ALUMINUM COVERED WITH ANODIC OXIDE-FILMS IN A NEUTRAL BORATE SOLUTION .1. THE MECHANISM OF RECTIFICATION [J].
TAKAHASHI, H ;
KASAHARA, K ;
FUJIWARA, K ;
SEO, M .
CORROSION SCIENCE, 1994, 36 (04) :677-+
[8]  
Vetter KJ, 1967, ELECTROCHEMICAL KINE, P183