LATTICE PARAMETERS OF MARTENSITE AND AUSTENITE IN FE-NI ALLOYS

被引:61
作者
REED, RP
SCHRAMM, RE
机构
[1] Cryogenics Division, National Bureau of Standards, Institute for Basic Standards, Boulder
关键词
D O I
10.1063/1.1658218
中图分类号
O59 [应用物理学];
学科分类号
摘要
The lattice parameters of the body-centered cubic phase (martensite) and the face-centered cubic phase (austenite) were determined for a series of FeSingle Bond signNi alloys. Compositions ranged from pure Fe to Fe-35 at.% Ni. Careful film and diffractometer Debye-Scherrer techniques on powder and bulk samples and computerized calculations and error analyses were employed. Results indicate that the martensite lattice parameter reaches a maximum between 10 and 20 at.% Ni and the room-temperature lattice parameter of the face-centered cubic phase has a maximum in alloys having greater than 35 at.% Ni. © 1969 The American Institute of Physics.
引用
收藏
页码:3453 / &
相关论文
共 25 条
[1]  
ABRAHAMSON EP, 1966, T METALL SOC AIME, V236, P76
[2]   A NEW REVERSIBLE SOLID-STATE TRANSFORMATION IN IRON-NICKEL ALLOYS IN INVAR RANGE OF COMPOSITONS [J].
ANANTHANARAYANAN, N ;
PEAVLER, RJ .
NATURE, 1961, 192 (480) :962-&
[3]  
BIBBY MJ, 1964, J IRON STEEL I, V202, P100
[4]  
Bradley AJ, 1937, PHILOS MAG, V23, P545
[5]  
BREEDIS JF, 1962, T METALL SOC AIME, V224, P1128
[6]   FAULTING IN DEFORMED AUSTENITE AND MARTENSITE [J].
GOLDMAN, AJ ;
WAGNER, CNJ .
ACTA METALLURGICA, 1963, 11 (04) :405-&
[7]  
GULJAEV AP, 1950, ZH TEKH FIZ, V20, P66
[8]  
HANSEN M, 1958, CONSTITUTION BINARY, P678
[9]  
Jette ER, 1936, T AM I MIN MET ENG, V120, P259
[10]  
KAEBLE EF, 1967, HANDBOOK XRAYS, P10