MICROHARDNESS INDENTATION APPLICATION AND LIMITATION IN FRACTURE-TOUGHNESS EVALUATION OF CERAMICS

被引:3
作者
NAYEBHASHEMI, H
TRACY, CA
机构
[1] Department of Mechanical Engineering, Northeastern University, Boston, 02115, MA
关键词
D O I
10.1007/BF02325995
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The use of a microhardness indentation as a controlled flaw in a flexural specimen for measuring fracture toughness in advanced ceramics is critically evaluated. From a review of fracture-toughness testing methodologies for ceramics it is shown that currently there are not any standardized or widely agreed upon K(Ic) test procedures. The problems associated with the controlled flaw test are discussed and analyzed. An experimental program is used to investigate the effects of residual stress on the measurement of fracture toughness in a wide variety of sintered and hot-pressed advanced ceramics including TiB2, Al2O3, SiC, ZrO2, Si3N4. The validity of the test procedure for evaluating K(Ic) of advanced ceramics in general is put forth.
引用
收藏
页码:366 / 372
页数:7
相关论文
共 17 条
[11]  
QUINN GD, 1986, J MAT SCI APR
[12]  
ROOKE DP, 1974, COMPENDIUM STRESS IN, P279
[14]  
TRACY C, 1988, ADV CERAMICS FRACTOG, V22
[15]  
TRACY CA, 1988, THESIS NE U
[16]   LINE-SPRING ANALYSIS OF THE DOUBLE-TORSION SPECIMEN [J].
WHITE, CS .
ENGINEERING FRACTURE MECHANICS, 1984, 19 (04) :751-753
[17]  
1983, MILSTD1942MR US ARM