SUPERCONDUCTING JOINTS FORMED BETWEEN POWDER-IN-TUBE Bi2Sr2Ca2Cu3Oz/Ag TAPES

被引:25
作者
Tkaczyk, J. E. [1 ]
Arendt, R. H. [1 ]
Bednarczyk, P. J. [1 ]
Garbauskas, M. F. [1 ]
Jones, B. A. [1 ]
Kilmer, R. J. [1 ]
Lay, K. W. [1 ]
机构
[1] GE, Corp Res & Dev, POB 8, Schenectady, NY 12301 USA
关键词
D O I
10.1109/77.233852
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
Superconducting joints between Ag clad, Bi2Sr2Ca2Cu3Oz tapes have been obtained with approximately 1/2 the current capacity of the tapes themselves. The Ag sheath is removed from one side of each tape without significantly disturbing the superconducting core. The exposed superconducting core of the two tapes are brought into contact and pressed so as to again seal the superconductor in a Ag sheath. Finally a reaction anneal is performed to join the two cores together and repair damage associated with the removal of Ag and the pressing. Transport measurements using multiple voltage taps have been found useful in characterizing the critical current variation across the joint.
引用
收藏
页码:946 / 948
页数:3
相关论文
共 5 条
  • [1] Lay K.W., P 1992 SPRING MAT RE
  • [2] Murayama Norimitsu, 1990, JPN J APPL PHYS, pL875
  • [3] DIFFUSION BONDING OF BI-PB-SR-CA-CU-O HIGH-TC SUPERCONDUCTORS
    MUTOH, Y
    INOUE, M
    KOMATSU, T
    [J]. JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1990, 29 (08): : L1432 - L1434
  • [4] Sato Ken-ichi, 1992, PHYSICA C, V190, P50
  • [5] MICROSTRUCTURAL STUDY OF BI(2223)/AG TAPES WITH JC(77-K, 0 T) VALUES OF UP TO 3.3X10(4)A CM-2
    YAMADA, Y
    OBST, B
    FLUKIGER, R
    [J]. SUPERCONDUCTOR SCIENCE & TECHNOLOGY, 1991, 4 (04) : 165 - 171