DEACTIVATION OF RUTHENIUM CATALYSTS IN CONTINUOUS GLUCOSE HYDROGENATION

被引:95
作者
ARENA, BJ
机构
[1] UOP, Des Plaines
关键词
CATALYST CHARACTERIZATION (AAS; XRD); DEACTIVATION; GLUCOSE HYDROGENATION; RUTHENIUM ALUMINA;
D O I
10.1016/0926-860X(92)80057-J
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Several Ru/Al2O3 glucose hydrogenation catalysts were tested in continuous operation. After use, spent catalysts were characterized by a variety of techniques to determine what changes had accompanied deactivation. The ruthenium tended to agglomerate, and changes in the physical properties of the Al2O3 support were observed. In addition, the buildup of iron, sulfur, and gluconic acid on the catalyst during use was detected. Experimental data strongly implicate these changes in causing catalyst deactivation. For example, when iron and gluconic acid poisoning is minimized, substantial improvements in catalyst stability are achieved.
引用
收藏
页码:219 / 229
页数:11
相关论文
共 11 条
  • [1] ALBERT R, 1981, CATALYSIS ORGANIC RE, P421
  • [2] Arena B. J., 1983, [No title captured], Patent No. [US 4,380,680, 4380680]
  • [3] DALLABETTA RA, 1974, J CATAL, V34, P57
  • [4] GITZEN WH, 1970, ALUMINA CERAMIC MATE
  • [5] GREEN JW, 1957, CARBOHYDRATES, P301
  • [6] LOHMAR RL, 1957, CARBOHYDRATES, P248
  • [7] SULFUR ON NOBLE-METAL CATALYST PARTICLES
    WANG, T
    VAZQUEZ, A
    KATO, A
    SCHMIDT, LD
    [J]. JOURNAL OF CATALYSIS, 1982, 78 (02) : 306 - 318
  • [8] WILT HGJ, 1972, IND ENG CHEM PROD RD, V11, P37
  • [9] HYDROGENATION OF GLUCOSE, FRUCTOSE, AND THEIR MIXTURES
    WISNIAK, J
    SIMON, R
    [J]. INDUSTRIAL & ENGINEERING CHEMISTRY PRODUCT RESEARCH AND DEVELOPMENT, 1979, 18 (01): : 50 - 57
  • [10] 1988, SRI CHEM EC HDB