GROWTH-CHARACTERISTICS OF PHOTOLYTIC LASER-INDUCED CHEMICAL VAPOR-DEPOSITION OF TUNGSTEN FROM WF6

被引:8
作者
MOGYOROSI, P
CARLSSON, JO
机构
[1] Uppsala Uninersitv. Department of Chpmixtrv, Thin Film and Surface Chemistrv Group, S-751 21, Uppsala
来源
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS | 1992年 / 10卷 / 05期
关键词
D O I
10.1116/1.577876
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
ArF laser induced chemical vapor deposition (CVD) of W onto (100)Si from a WF6/H2/Ar mixture and with the laser beam in parallel to the substrate surface was studied. The influence of substrate temperature on the deposition rate was investigated in a broad range (25-450-degrees-C) for both focused and unfocused beam conditions and compared with thermal CVD data. Above the threshold temperature for the thermal process, 250-degrees-C, a combined thermal and photolytic process takes place. Below 250-degrees-C the laser induced photolytic process yields deposition with a nearly temperature independent deposition rate of about 100 angstrom/min when a focused beam is used. For an unfocused beam a slightly lower deposition rate was observed. The distance between the laser beam and the substrate surface had only a slight influence on the deposition rate. For the focused beam conditions the deposition rate was only reduced by roughly 10% when the distance was increased from 0 to 8 mm. For the unfocused case the deposition rate increased, without reaching the focused beam values, upon increasing the beam to substrate distance in the range 0-8 mm. The substrate temperature had a strong influence on the resistivity of the deposited films for both laser-induced and thermal processes. For obtaining a low resistivity value, 8-mu-OMEGA cm, a substrate temperature above 350-degrees-C was required. This was mainly due to the fact that the high-resistivity beta-phase was formed at lower temperatures. The influence of H-2 concentration on the growth rate was investigated by replacing H-2 with Ar. A small amount of H-2 was enough to increase the deposition rate considerably. Use of Ar diluted gas resulted also in a higher deposition rate. Finally, the deposition rate increased linearly with increased total pressure.
引用
收藏
页码:3131 / 3135
页数:5
相关论文
共 14 条
[2]   COMPARISON OF LASER-INITIATED AND THERMAL CHEMICAL VAPOR-DEPOSITION OF TUNGSTEN FILMS [J].
DEUTSCH, TF ;
RATHMAN, DD .
APPLIED PHYSICS LETTERS, 1984, 45 (06) :623-625
[3]  
ERIKSSON TA, UNPUB
[4]  
HESZLER P, IN PRESS
[5]   SOME CONSIDERATIONS OF THE THERMODYNAMICS AND KINETICS OF THE CHEMICAL VAPOR-DEPOSITION OF TUNGSTEN [J].
HITCHMAN, ML ;
JOBSON, AD ;
KWAKMAN, LFT .
APPLIED SURFACE SCIENCE, 1989, 38 (1-4) :312-337
[6]   PLASMA-ENHANCED CHEMICAL VAPOR-DEPOSITION OF LOW-RESISTIVE TUNGSTEN THIN-FILMS [J].
KIM, YT ;
MIN, SK ;
HONG, JS ;
KIM, CK .
APPLIED PHYSICS LETTERS, 1991, 58 (08) :837-839
[8]  
KRANS RL, 1990, MATER RES SOC SYMP P, V181, P597, DOI 10.1557/PROC-181-597
[9]   EVALUATION OF LASER CVD TUNGSTEN FOR GATE ELECTRODE [J].
MATSUHASHI, H ;
NISHIKAWA, S ;
OHNO, S .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS & EXPRESS LETTERS, 1988, 27 (11) :L2161-L2163
[10]  
MATSUHASHI H, 1989, MAT RES S C, V129, P63