共 28 条
[2]
CREEP DEFORMATION OF CD AND HG AT LIQUID HELIUM TEMPERATURES
[J].
ACTA METALLURGICA,
1969, 17 (05)
:687-&
[3]
THE INSTABILITY OF PLASTIC FLOW OF METALS AT VERY LOW TEMPERATURES
[J].
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES,
1957, 240 (1221)
:229-242
[4]
THERMALLY-ACTIVATED GLIDE IN MAGNESIUM CRYSTALS FROM 4.2-DEGREES-K TO 420-DEGREES-K
[J].
PHILOSOPHICAL MAGAZINE,
1961, 6 (62)
:177-188
[5]
HYDROGEN CONTAMINATION IN TANTALUM AND NIOBIUM FOLLOWING UHV-DEGASSING
[J].
SCRIPTA METALLURGICA,
1972, 6 (11)
:1065-&
[6]
STRESS RELAXATION IN ZONE REFINED TUNGSTEN AND QUANTUM MECHANICAL TUNNELING OF DISLOCATIONS
[J].
ACTA METALLURGICA,
1971, 19 (03)
:223-&
[8]
GINDIN IA, 1963, PHYS MET METALLOGR, V15, P80
[9]
THE CREEP OF CADMIUM CRYSTALS AT LIQUID HELIUM TEMPERATURES
[J].
PHILOSOPHICAL MAGAZINE,
1956, 1 (05)
:400-408
[10]
LOW TEMPERATURE PLASTIC INSTABILITY IN PURE NIOBIUM SINGLE CRYSTALS
[J].
PHILOSOPHICAL MAGAZINE,
1971, 24 (188)
:437-&