共 9 条
[4]
Crystalline structure of heat-treated Scots pine[Pinus sylvestris L.] and Uluda? fir[Abies nordmanniana (Stev.) subsp. bornmuelleriana (Mattf.)] wood[J] . Wood Science and Technology . 2007 (3)
[6]
The water absorption of sapwood and heartwood of Scots pine and Norway spruce heat-treated at 170 ° C, 190 ° C, 210 ° C and 230 ° C[J] . Holz als Roh- und Werkstoff . 2006 (3)
[7]
Chemical changes in hydrothermal treated wood: FTIR analysis of combined hydrothermal and dry heat-treated wood[J] . B. F. Tjeerdsma,H. Militz.Holz als Roh- und Werkstoff . 2005 (2)
[9]
Modification of mass transfer properties in poplar wood ( P. robusta ) by a thermal treatment at high temperature[J] . P. Rousset,P. Perré,P. Girard.Holz als Roh- und Werkstoff . 2004 (2)