共 12 条
[1]
Liquid-phase aluminizing and siliconizing at the surface of a Ti60 alloy and improvement in oxidation resistance.[J].Hua-Ping Xiong;Wei Mao;Wen-Li Ma;Yong-Hui Xie;Yun-Feng Chen;Hong Yuan;Xiao-Hong Li.Materials Science & Engineering A.2006, 1
[2]
Durability of Cu–Al coating on Ti–6Al–4V substrate under fretting fatigue.[J].O. Jin;S. Mall;J.H. Sanders;S.K. Sharma.Surface & Coatings Technology.2006, 3
[3]
Coatings on Ti6Al4V as palliatives for fretting fatigue in cryogenic environment.[J].I. Caron;R. Gras;T. Ganne;J.M. De Monicault.Tribology International.2006, 10
[4]
Characteristics of the Ti 2 N layer produced by an ion assisted deposition method.[J].C Ruset;E Grigore;G.A Collins;K.T Short;F Rossi;N Gibson;H Dong;T Bell.Surface & Coatings Technology.2003,
[6]
Effect of various surface conditions on fretting fatigue behavior of Ti–6Al–4V.[J].A.L Hutson;M Niinomi;T Nicholas;D Eylon.International Journal of Fatigue.2002, 12