The molar heat capacity of hydrous copper chloride: Atacamite Cu2Cl(OH)(3)

被引:8
作者
Bisengalieva, MR
Kiseleva, IA
Melchakova, LV
Ogorodova, LP
Gurevich, AM
机构
[1] MOSCOW MV LOMONOSOV STATE UNIV, DEPT GEOL, MOSCOW 119899, RUSSIA
[2] KAZAKH ACAD SCI, INST CHEM MET, KARAGANDA 470032, KAZAKHSTAN
[3] UKRAINIAN ACAD SCI, INST LOW TEMP ENGN PHYS, UA-310164 KHARKOV, UKRAINE
关键词
calorimetry; entropy; heat capacity; atacamite;
D O I
10.1006/jcht.1996.0162
中图分类号
O414.1 [热力学];
学科分类号
摘要
The heat capacity of natural atacamite has been measured between T = 2 K and T = 305 K by cryogenic-adiabatic calorimetry. At T = 298.15 K, the standard molar heat capacity C(p,m)degrees and entropy S-m degrees for atacamite are (19.16 +/- 0.07).R and (20.18 +/- 0.08).R (where R = 8.3144 J.K-1.mol(-1)), respectively. The heat capacity exibits anomalous behaviour at temperatures lower than 10.5 K. Smoothed thermodynamic properties: molar heat capacity; molar entropy increment Delta(0)(T)S(m) degrees; and (Phi(m) degrees + Delta(0)(T)H(m) degrees/T), where T = 298.15 K, have been calculated. Between T = 290 K and T = 508 K the heat capacity of atacamite measured by d.s.c. is represented by the equation: C(p,m)degrees/R = 18.80 + 8.11.10(-3).(T/K) - 1.87.10(-5).(K/T)(2). (C) 1997 Academic Press Limited.
引用
收藏
页码:345 / 352
页数:8
相关论文
共 23 条
[1]  
ALAPINA AV, 1976, THERMAL PHYSICAL PRO, V9, P113
[2]  
[Anonymous], 1964, STABILITY CONSTANTS
[3]  
BARTON PB, 1960, AM J SCI, V258, P21
[4]  
BEREZOVSKII GA, 1987, THERMODYNAMICS PROPE
[5]  
BISENGALIEVA MR, 1993, VESTN MOSK U G, V2, P38
[6]  
BISENGALIEVA MR, 1990, MINERALOG ZH, V12, P51
[7]  
Feitknecht W., 1963, Pure Appl. Chem, V6, P130
[8]  
Glushko V.P., 1972, THERMAL CONSTANTS SU, VVI
[9]  
IORISH VS, 1986, ZH FIZ KHIM+, V60, P2583
[10]  
Kasatov B.K., 1974, Thermal analysis of minerals and rocks