Process simulation based life cycle assessment of cyanide-free refractory gold concentrate processing - Case study: Cupric chloride leaching

被引:14
作者
Elomaa, Heini [1 ]
Rintala, Lotta [2 ]
Aromaa, Jari [1 ]
Lundstrom, Mari [1 ]
机构
[1] Aalto Univ, Sch Chem Engn, Dept Chem & Met Engn, Vuorimiehentie 2,POB 16200, FI-00076 Aalto, Finland
[2] VTT Tech Res Ctr Finland Ltd, Solut Nat Resources & Environm, Vuorimiehentie 2,POB 1000, FI-02044 Espoo, Finland
基金
芬兰科学院;
关键词
Gold leaching; Cyanide-free; CuCl2; HSC-Sim; Sustainable gold processing; METAL PRODUCTION; COPPER; EXTRACTION; MECHANISM; KINETICS; INDUSTRY; SILVER;
D O I
10.1016/j.mineng.2020.106559
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The development of cyanide-free gold leaching methods is becoming increasingly important due to the treatment of complex ores, where treatment by cyanidation is not economically viable. Cupric chloride leaching provides an alternative leaching process to replace cyanidation. A detailed simulation of refractory gold concentrate processing by cupric chloride leaching is presented in this study. The simulation with mass and energy balances was built to be used as life cycle inventory data to evaluate the environmental impacts of the development stage cupric chloride process. Three cases, the Base Case (125 g/L Cl-), Mild Case (50 g/L Cl-), and Extremely Mild Case (20 g/L Cl-), were investigated in two flowsheet options. Loss of gold to wash waters was observed in the Flowsheet 1 cases, and therefore Flowsheet 2, with the recirculation of wash water to solvent extraction, was developed and investigated in order to achieve higher gold recovery. The gold extraction improved from around 85% to 99%. Chemical consumption (NaCl, NaBr, CuCl2) was greatly affected by the leaching conditions, higher concentrations consuming more initial chemicals. In milder conditions, efficient recycling of chlorides could be obtained in the process, and no addition of NaCl was required. In the Extremely Mild Case, the chloride concentration was close to sea water conditions (20 g/L), where sea water could be used to provide chlorides for the process, and the effluent waters could be disposed of in the sea after purification. The global warming potential was estimated to be 12.5 t CO2-e/kg Au in chloride leaching and was further decreased to 10.6 t CO2-e/kg Au in the mildest conditions (20 g/L Cl-). The milder chloride leaching conditions (20 g/L Cl - and 50 g/L Cl-) were shown to decrease the acidification potential, eutrophication potential, and water depletion.
引用
收藏
页数:12
相关论文
共 65 条
  • [1] Cyanide-free gold leaching in exceptionally mild chloride solutions
    Ahtiainen, Riina
    Lundstrom, Mari
    [J]. JOURNAL OF CLEANER PRODUCTION, 2019, 234 : 9 - 17
  • [2] Preg-robbing verification and prevention in gold chloride-bromide leaching
    Ahtiainen, Riina
    Lundstrom, Mari
    Liipo, Jussi
    [J]. MINERALS ENGINEERING, 2018, 128 : 153 - 159
  • [3] PREG-ROBBING OF GOLD IN CHLORIDE-BROMIDE SOLUTION
    Ahtiainen, Riina
    Lundstrom, Mari
    [J]. PHYSICOCHEMICAL PROBLEMS OF MINERAL PROCESSING, 2016, 52 (01): : 244 - 251
  • [4] Effect of biological pretreatment on metal extraction from flotation tailings for chloride leaching
    Altinkaya, Pelin
    Makinen, Jarno
    Kinnunen, Paivi
    Kolehmainen, Eero
    Haapalainen, Mika
    Lundstrom, Mari
    [J]. MINERALS ENGINEERING, 2018, 129 : 47 - 53
  • [5] [Anonymous], 2006, ISO 14040 2006 ENV M
  • [6] [Anonymous], 2006, Environmental Management: Life Cycle Assessment
  • [7] Principles and Framework
  • [8] Aylmore MG, 2016, GOLD ORE PROCESSING: PROJECT DEVELOPMENT AND OPERATIONS, 2ND EDITION, P447, DOI 10.1016/B978-0-444-63658-4.00027-X
  • [9] Thiosulfate leaching of gold - A review
    Aylmore, MG
    Muir, DM
    [J]. MINERALS ENGINEERING, 2001, 14 (02) : 135 - 174
  • [10] Dai Y, 2013, IEEE C ELECTR PERFOR, P61, DOI 10.1109/EPEPS.2013.6703467