Biodegradable bone cement compositions based on acrylate and epoxide terminated poly(propylene fumarate) oligomers and calcium salt compositions

被引:73
作者
Domb, AJ
Manor, N
Elmalak, O
机构
[1] Hebrew University of Jerusalem, Sch. of Pharmacy-Faculty of Medicine, Dept. of Pharmaceutical Chemistry
关键词
bone cement; biodegradable polymers; poly(propylene fumarate); polymer composites;
D O I
10.1016/0142-9612(96)89657-8
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The synthesis of biodegradable bone cement compositions is presented. These bone cement compositions can be applied as a putty-like mixture and harden to a strong material in a bone fracture. They degrade from the site of application to allow the ingrowth of new bone for complete healing of the bone fracture. The bone cement is composed of a solid particulate phase dispersed in an initially liquid polymeric phase, which can be hardened by cross-linking. The polymeric phase is a low-molecular-weight liquid poly(propylene fumarate) (PPF) containing double bonds available for crosslinking. The solid particulate phase consists of calcium carbonate and tricalcium phosphate. PPF oligomers of M(w) = 1800 and M(n) = 750 were prepared from the condensation of non-volatile bis(2-hydroxypropyl fumarate) and propylene-bis(hydrogen maleate) trimers. PPF terminated divinyl and diepoxide derivatives were obtained from the reactions between PPF diol and acryloyl chloride or epichlorhydrin, respectively. Putty-like cement compositions were prepared from a mixture of 30 wt% polymer phase containing benzoyl peroxide-dimethyl toluidine as polymerization catalyst and 70 wt% calcium salts. The divinyl and diepoxide terminated PPF oligomers provided a high strength composition of between 30 and 129 MPa which is suitable for bone cement applications. In vitro hydrolysis of the composites showed little weight loss with the compressive strength remaining above 20 MPa after 4 weeks in buffer solution. Compositions of the PPF oligomers cross-linked without calcium salts showed a gradual weight loss (10-65 wt% after 4 weeks) when placed in buffer solution followed by high water absorption (18-200 wt% after 4 weeks), with the epoxide terminated PPF being the least to degrade or absorb water.
引用
收藏
页码:411 / 417
页数:7
相关论文
共 14 条
  • [1] BONE COMPRESSIVE STRENGTH - INFLUENCE OF DENSITY AND STRAIN RATE
    CARTER, DR
    HAYES, WC
    [J]. SCIENCE, 1976, 194 (4270) : 1174 - 1176
  • [2] Domb A. J., 1989, U. S. Patent, Patent No. [4,888,413, 4888413]
  • [3] THE FORMATION OF PROPYLENE FUMARATE OLIGOMERS FOR USE IN BIOERODIBLE BONE-CEMENT COMPOSITES
    DOMB, AJ
    LAURENCIN, CT
    ISRAELI, O
    GERHART, TN
    LANGER, R
    [J]. JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1990, 28 (05) : 973 - 985
  • [4] DREYFFUS P, 1969, RING OPENING POLYM
  • [5] INVITRO CHARACTERIZATION AND BIOMECHANICAL OPTIMIZATION OF A BIODEGRADABLE PARTICULATE COMPOSITE BONE-CEMENT
    GERHART, TN
    MILLER, RL
    KLESHINSKI, SJ
    HAYES, WC
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1988, 22 (11): : 1071 - 1082
  • [6] INVIVO HISTOLOGIC AND BIOMECHANICAL CHARACTERIZATION OF A BIODEGRADABLE PARTICULATE COMPOSITE BONE-CEMENT
    GERHART, TN
    RENSHAW, AA
    MILLER, RL
    NOECKER, RJ
    HAYES, WC
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1989, 23 (01): : 1 - 16
  • [7] THE MECHANICAL-PROPERTIES OF HUMAN TIBIAL TRABECULAR BONE AS A FUNCTION OF METAPHYSEAL LOCATION
    GOLDSTEIN, SA
    WILSON, DL
    SONSTEGARD, DA
    MATTHEWS, LS
    [J]. JOURNAL OF BIOMECHANICS, 1983, 16 (12) : 965 - 969
  • [8] IBAY AC, 1985, POLYM MAT SCI ENG, V53, P505
  • [9] BIODEGRADATION BEHAVIOR OF VARIOUS CALCIUM-PHOSPHATE MATERIALS IN BONE TISSUE
    KLEIN, CPAT
    DRIESSEN, AA
    DEGROOT, K
    VANDENHOOFF, A
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1983, 17 (05): : 769 - 784
  • [10] MARK HF, 1969, ENCY POLYM SCI TECHN, V11, P134