Adsorption of spillover hydrogen atoms on single-wall carbon nanotubes

被引:133
作者
Yang, FH [1 ]
Lachawiec, AJ [1 ]
Yang, RT [1 ]
机构
[1] Univ Michigan, Dept Chem Engn, Ann Arbor, MI 48109 USA
关键词
D O I
10.1021/jp056461u
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Spillover of hydrogen on nanostructured carbons is a phenomenon that is critical to understand in order to produce efficient hydrogen storage adsorbents for fuel cell applications. The spillover and interaction of atomic hydrogen with single-walled carbon nanotubes (SWNTs) is the focus of this combined theoretical and experimental work. To understand the spillover mechanism, very low occupancies (i.e., 1 and 2 H atoms adsorbed) on (5,0), (7,0), (9,0) zigzag (semiconducting) SWNTs and a (5,5) anrichair (metallic) SWNT, with corresponding diameters of 3.9. 5.5, 7.0, and 6.8 angstrom, were investigated. The adsorption binding energy of H atoms depends on H occupancy, tube diameter, and helicity (or chirality), as well as endohedral (interior) vs exohedral (exterior) binding. Exohedral binding energies are substantially higher than endohedral binding energies due to easier sp(2)-sp(3) transition in hybridization of carbon on exterior walls upon binding. A binding energy as low as -8.9 kcal/mol is obtained for 2H atoms on the exterior wall of a (5, 0) SWNT. The bindiner energies of H atoms on the metallic SWNT are significantly weaker (about 23 kcal/mol weaker) than that on the semiconductor SWNT, for both endohedral and exohedral adsorption. The binding energy is generally higher on SWNTs of larger diameters, while its dependence on H occupancy is relatively weak except at very low occupancies. Experimental results at 298 K and for pressures up to 10 MPa with a carbon-bridged composite material containing SWNTs demonstrate the presence of multiple adsorption sites based on desorption hysteresis for the spiltover H on SWNTs, and the experimental results were in qualitative agreement with the molecular orbital calculation results.
引用
收藏
页码:6236 / 6244
页数:9
相关论文
共 63 条
[1]   Hydrogen desorption and adsorption measurements on graphite nanofibers [J].
Ahn, CC ;
Ye, Y ;
Ratnakumar, BV ;
Witham, C ;
Bowman, RC ;
Fultz, B .
APPLIED PHYSICS LETTERS, 1998, 73 (23) :3378-3380
[2]  
Alonso JA, 2004, IEEE T NANOTECHNOL, V3, P304, DOI [10.1109/TNANO.2004.828678, 10.1109/tnano.2004.828678]
[3]  
Bauschlicher CW, 2002, NANO LETT, V2, P337, DOI [10.1021/nl020283o, 10.1021/n1020283o]
[4]  
Bauschlicher CW, 2001, NANO LETT, V1, P223, DOI [10.1021/nl010018n, 10.1021/n1010018n]
[5]   Hydrogen and fluorine binding to the sidewalls of a (10,0) carbon nanotube [J].
Bauschlicher, CW .
CHEMICAL PHYSICS LETTERS, 2000, 322 (3-4) :237-241
[6]   DENSITY-FUNCTIONAL THERMOCHEMISTRY .3. THE ROLE OF EXACT EXCHANGE [J].
BECKE, AD .
JOURNAL OF CHEMICAL PHYSICS, 1993, 98 (07) :5648-5652
[7]   DENSITY-FUNCTIONAL THERMOCHEMISTRY .3. THE ROLE OF EXACT EXCHANGE [J].
BECKE, AD .
JOURNAL OF CHEMICAL PHYSICS, 1993, 98 (07) :5648-5652
[8]   DENSITY-FUNCTIONAL EXCHANGE-ENERGY APPROXIMATION WITH CORRECT ASYMPTOTIC-BEHAVIOR [J].
BECKE, AD .
PHYSICAL REVIEW A, 1988, 38 (06) :3098-3100
[9]   Studies into the storage of hydrogen in carbon nanofibers: Proposal of a possible reaction mechanism [J].
Browning, DJ ;
Gerrard, ML ;
Lakeman, JB ;
Mellor, IM ;
Mortimer, RJ ;
Turpin, MC .
NANO LETTERS, 2002, 2 (03) :201-205
[10]   Model of micropore closure in hard carbon prepared from sucrose [J].
Buiel, ER ;
George, AE ;
Dahn, JR .
CARBON, 1999, 37 (09) :1399-1407