Composition, structure, stress, and coercivity of electrodeposited soft magnetic CoNiFe films - Thickness and substrate dependence

被引:113
作者
Tabakovic, I [1 ]
Inturi, V [1 ]
Riemer, S [1 ]
机构
[1] Seagate Technol, Bloomington, MN 55435 USA
关键词
D O I
10.1149/1.1421346
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The properties of soft magnetic CoNiFe films electrodeposited in the presence of saccharin and sodium lauryl sulfate additives were studied in terms of their thickness and substrate dependence. Auger depth profile analysis of the elemental composition in CoNiFe films electrodeposited over different substrates (Pd90Ni10, 1.0 T NiFe, Cu) demonstrate that the average composition at the substrate interface and bulk deposited films remains constant. X-ray diffraction (XRD) measurements reveal the existance of mixed fcc + bcc phase with larger amounts of bcc crystallites near the substrate side of the films, i.e., at the lower thickness. XRD and transmission electron microscopy measurements revealed a larger grain size at the CoNiFe/substrate interface. The measured average stress is both substrate- and thickness-dependent. The easy-axis coercivity, H-c, follows the Neel's relation H-c = ct(n) (t is the thickness and c is a constant). It was found that the value of the exponent n is substrate dependent. Mechanisms related to the coercivity of CoNiFe films deposited over different substrates (1.0 T NiFe, Cu, Pd90Ni10, high magnetic moment CoNiFe) are discussed in terms of material properties of these magnetic films. (C) 2001 The Electrochemical Society.
引用
收藏
页码:C18 / C22
页数:5
相关论文
共 27 条
[1]   Future directions in electroplated materials for thin-film recording heads [J].
Andricacos, PC ;
Robertson, N .
IBM JOURNAL OF RESEARCH AND DEVELOPMENT, 1998, 42 (05) :671-680
[2]  
ANDRICACOS PC, 1994, ADV ELEC SC, V3, P227
[3]   Soft to hard magnetic anisotropy in nanostructured magnets [J].
Arcas, J ;
Hernando, A ;
Barandiaran, JM ;
Prados, C ;
Vazquez, M ;
Marin, P ;
Neuweiler, A .
PHYSICAL REVIEW B, 1998, 58 (09) :5193-5196
[4]  
CHANG JW, 1992, MAGNETIC MAT PROCESS, P315
[5]   VARIATION OF COMPOSITION WITH THICKNESS IN THIN ELECTRODEPOSITED FILMS OF NICKEL-IRON ALLOYS [J].
COCKETT, GH ;
SPENCERTIMMS, ES .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1961, 108 (09) :906-908
[6]   Huge magnetic hardening ascribed to metastable crystallites during first stages of devitrification of amorphous FeSiBNbSn alloys [J].
Cremaschi, V ;
Arcondo, B ;
Sirkin, H ;
Vázquez, M ;
Asenjo, A ;
Garcia, JM ;
Abrosimova, G ;
Aronin, A .
JOURNAL OF MATERIALS RESEARCH, 2000, 15 (09) :1936-1942
[7]   Grain size internal stress relationship in iron-nickel alloy electrodeposits [J].
Czerwinski, F .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (10) :3327-3332
[8]  
DAHMS H, 1966, ELECTROCHEM TECHNOL, V4, P530
[9]  
Djokic SS, 1992, MOD ASPECT ELECTROC, P417, DOI 10.1007/978-1-4615-3376-4_4
[10]   MAGNETIZATION AND SWITCHING CHARACTERISTICS OF COMPOSITE THIN MAGNETIC FILMS [J].
GOTO, E ;
HAYASHI, N ;
MIYASHIT.T ;
NAKAGAWA, K .
JOURNAL OF APPLIED PHYSICS, 1965, 36 (09) :2951-&