Plasma-polymerised coatings used as pre-treatment for aluminium alloys

被引:33
作者
Fernandes, JCS [1 ]
Ferreira, MGS
Haddow, DB
Goruppa, A
Short, R
Dixon, DG
机构
[1] Inst Super Tecn, Dept Chem Engn, P-1049001 Lisbon, Portugal
[2] Univ Sheffield, Dept Mat Engn, Sheffield S1 3JD, S Yorkshire, England
[3] Adv Technol Ctr Sowerby, Bristol BS34 7QW, Avon, England
关键词
plasma polymerisation; aluminium alloy; adhesion; corrosion;
D O I
10.1016/S0257-8972(01)01705-4
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The pre-treatment of aluminium alloys prior to painting or adhesive bonding is an essential technology in many industrial sectors (e.g. aerospace industry). However, the pre-treatments used on the substrates, which are vital to ensure reliable long-term performance, often comprise a range of environmentally objectionable chemicals, such as solvents and chromates, some of which are carcinogenic. The plasma deposition of thin coatings on aluminium, which exhibit strong interfacial bonding, could be an alternative to the traditional chromate-based treatments. It is envisaged that in a single plasma reactor, plasma cleaning, etching and deposition could provide a complete preparation cycle before painting, avoiding the use, handling and disposal of hazardous materials. In the present work, the corrosion behaviour and adhesive joint performance of plasma-coated Alclad AA2024-T3 alloy were investigated. The coatings were deposited from hexamethyldisiloxane monomer (HMDSO) in a capacitively coupled RF plasma reactor. The same evaluations were carried out on specimens painted with an epoxy primer after coating deposition. The coatings conferred protection against corrosion and provided a good interface for strong, durable adhesive bonds. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:8 / 13
页数:6
相关论文
共 26 条
[1]   An X-ray photoelectron spectroscopic investigation into the chemical structure of deposits formed from hexamethyldisiloxane/oxygen plasmas [J].
Alexander, MR ;
Short, RD ;
Jones, FR ;
Stollenwerk, M ;
Zabold, J ;
Michaeli, W .
JOURNAL OF MATERIALS SCIENCE, 1996, 31 (07) :1879-1885
[2]   The role of precipitates enriched with copper on the susceptibility to pitting corrosion of the 2024 aluminium alloy [J].
Blanc, C ;
Lavelle, B ;
Mankowski, G .
CORROSION SCIENCE, 1997, 39 (03) :495-510
[3]   Local dissolution phenomena associated with S phase (Al2CuMg) particles in aluminum alloy 2024-T3 [J].
Buchheit, RG ;
Grant, RP ;
Hlava, PF ;
Mckenzie, B ;
Zender, GL .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (08) :2621-2628
[4]   Relation between microstructural aspects of AA2024 and its corrosion behaviour investigated using AFM scanning potential technique [J].
Campestrini, P ;
van Westing, EPM ;
van Rooijen, HW ;
de Wit, JHW .
CORROSION SCIENCE, 2000, 42 (11) :1853-1861
[5]   Microconstituent-induced pitting corrosion in aluminum alloy 2024-T3 [J].
Chen, GS ;
Gao, M ;
Wei, RP .
CORROSION, 1996, 52 (01) :8-15
[6]  
FERNANDES JSC, 1998, D701 ISTLISB
[7]  
Grundmeier G, 1998, MATER CORROS, V49, P150, DOI 10.1002/(SICI)1521-4176(199803)49:3<150::AID-MACO150>3.0.CO
[8]  
2-X
[9]   Interfacial processes during plasma polymer deposition on oxide covered iron [J].
Grundmeier, G ;
Stratmann, M .
THIN SOLID FILMS, 1999, 352 (1-2) :119-127
[10]   Better aluminium mirrors by integrating plasma pretreatment, sputtering, and plasma polymerization for large-scale car headlight production [J].
Grünwald, H ;
Adam, R ;
Bartella, J ;
Jung, M ;
Dicken, W ;
Kunkel, S ;
Nauenburg, K ;
Gebele, T ;
Mitzlaff, S ;
Ickes, G ;
Patz, U ;
Snyder, J .
SURFACE & COATINGS TECHNOLOGY, 1999, 111 (2-3) :287-296