Continuous distribution kinetics for the thermal degradation of LDPE in solution

被引:14
作者
Kumar, GS [1 ]
Kumar, VR [1 ]
Madras, G [1 ]
机构
[1] Indian Inst Sci, Dept Chem Engn, Bangalore 560012, Karnataka, India
关键词
low-density polyethylene; degradation; continuous kinetics; solution; weak links;
D O I
10.1002/app.2344
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Polymer degradation in solution has several advantages over melt pyrolysis, The degradation of low-density polyethylene (LDPE) occurs at much lower temperatures in solution (280-360degreesC) than in conventional melt pyrolysis (400-450degreesC). The thermal degradation kinetics of LDPE in solution was investigated in this work. LDPE was dissolved in liquid paraffin and degraded for 3 h at various temperatures (280-360degreesC). Samples were taken at specific times and analyzed with high-pressure liquid chromatography/gel permeation chromatography for the molecular weight distribution (MWD), The time evolution of the MWD was modeled with continuous distribution kinetics. Data indicated that LDPE followed random-chain-scission degradation. The rapid initial drop in molecular weight, observed up to 45 min, was attributed to the presence of weak links in the polymer. The rate coefficients for the breakage of weak and strong links were determined, and the corresponding average activation energies were calculated to be 88 and 24 kJ/mol, respectively. (C) 2002 John Wiley Sons, Inc.
引用
收藏
页码:681 / 690
页数:10
相关论文
共 33 条
[1]   Transformation of several plastic wastes into fuels by catalytic cracking [J].
Arandes, JM ;
Abajo, I ;
LopezValerio, D ;
Fernandez, I ;
Azkoiti, MJ ;
Olazar, M ;
Bilbao, J .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1997, 36 (11) :4523-4529
[2]   ON THEORY OF REACTIONS IN CONTINUOUS MIXTURES [J].
ARIS, R ;
GAVALAS, GR .
PHILOSOPHICAL TRANSACTIONS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1966, 260 (1112) :351-&
[3]  
CHART J, 1997, POLYM DEGRADATION ST, V57, P135
[4]  
CHART JH, 1997, POLYM DEGRAD STABIL, V57, P113
[5]  
CHENG Z, 1990, J PHYS A, V73, P1233
[6]   WEAK LINKS IN POLYSTYRENE [J].
CHIANTORE, O ;
CAMINO, G ;
COSTA, L .
POLYMER DEGRADATION AND STABILITY, 1981, 3 (03) :209-219
[7]   Recycled plastics in FCC feedstocks: Specific contributions [J].
delaPuente, G ;
Arandes, JM ;
Sedran, UA .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1997, 36 (11) :4530-4534
[8]   Waxy polyethylenes from solution thermolysis of high density polyethylene: inert and H-donor solvent dilution effect [J].
Guy, L ;
Fixari, B .
POLYMER, 1999, 40 (10) :2845-2857
[9]   CATALYTIC DECOMPOSITION OF POLYETHYLENE USING A TUBULAR FLOW REACTOR SYSTEM [J].
ISHIHARA, Y ;
NANBU, H ;
IKEMURA, T ;
TAKESUE, T .
FUEL, 1990, 69 (08) :978-984
[10]   Distribution kinetics of radical mechanisms: Reversible polymer decomposition [J].
Kodera, Y ;
McCoy, BJ .
AICHE JOURNAL, 1997, 43 (12) :3205-3214