Do Directional Primary and Secondary Crack Patterns in Thin Films of Maghemite Nanocrystals Follow a Universal Scaling Law?

被引:15
作者
Ngo, Anh Tu [1 ]
Richardi, Johannes [1 ]
Pileni, Marie Paule [1 ]
机构
[1] Univ Paris 06, CNRS, Lab Mat Mesoscop & Nanometr LM2N, UMR 7070, F-75252 Paris 05, France
关键词
D O I
10.1021/jp802736g
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cracks due to a shrinking film restricted by adhesion to a surface are observed in nature at various length scales ranging from tiny crack segments in nanoparticle films to enormous domains observed in the earth's crust. Here, we study the formation of cracks in magnetic films made of maghemite (gamma-Fe2O3) nanocrystals. The cracks are oriented by an external magnetic field applied during the drying process which presents a new method to produce directional crack patterns. It is shown that directional and isotropic crack patterns follow the same universal scaling law with the film height varying from micrometer to centimeter scales. Former experimental studies of scaling laws were limited to small variations in height (1 order of magnitude). The large variation in height in our expriments becomes possible due to the combined use of nanocrystals and electron microscopy. A simple two-dimensional computer model for elastic fracture leads to structural and scaling behaviors, which match those observed in the experiments.
引用
收藏
页码:14409 / 14414
页数:6
相关论文
共 21 条
[1]   REGULAR PATTERNS OF CRACKS FORMED BY DIRECTIONAL DRYING OF A COLLOIDAL SUSPENSION [J].
ALLAIN, C ;
LIMAT, L .
PHYSICAL REVIEW LETTERS, 1995, 74 (15) :2981-2984
[2]  
[Anonymous], 1986, NUMERICAL RECIPES C
[3]  
BELOUSSOV VV, 1965, PHYS CHEM EARTH, V6, P409
[4]   Experimental model of cracking induced by drying shrinkage [J].
Colina, H ;
Roux, S .
EUROPEAN PHYSICAL JOURNAL E, 2000, 1 (2-3) :189-194
[5]   Flow and fracture in drying nanoparticle suspensions [J].
Dufresne, ER ;
Corwin, EI ;
Greenblatt, NA ;
Ashmore, J ;
Wang, DY ;
Dinsmore, AD ;
Cheng, JX ;
Xie, XS ;
Hutchinson, JW ;
Weitz, DA .
PHYSICAL REVIEW LETTERS, 2003, 91 (22)
[6]   AN EXPERIMENTAL-STUDY OF CRACKING INDUCED BY DESICCATION [J].
GROISMAN, A ;
KAPLAN, E .
EUROPHYSICS LETTERS, 1994, 25 (06) :415-420
[7]   ULTRAFINE MAGHEMITE PARTICLES .1. STUDIES OF INDUCED MAGNETIC TEXTURE [J].
HENDRIKSEN, PV ;
BODKER, F ;
LINDEROTH, S ;
WELLS, S ;
MORUP, S .
JOURNAL OF PHYSICS-CONDENSED MATTER, 1994, 6 (16) :3081-3090
[8]   Patterns and scaling in surface fragmentation processes [J].
Hornig, T ;
Sokolov, IM ;
Blumen, A .
PHYSICAL REVIEW E, 1996, 54 (04) :4293-4298
[9]  
ISRAELACHVILI J, 2007, SPRINGER HDB NANOTEC, P1
[10]   Pattern selection of cracks in directionally drying fracture [J].
Komatsu, TS ;
Sasa, SI .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1997, 36 (1A) :391-395