Synthesis of nanosized titanium powder by high energy milling

被引:28
作者
Dabhade, VV [1 ]
Mohan, TRR [1 ]
Ramakrishnan, P [1 ]
机构
[1] Indian Inst Technol, Dept Met Engn & Mat Sci, Bombay 400076, Maharashtra, India
关键词
nanosize; titanium; attrition milling;
D O I
10.1016/S0169-4332(01)00456-1
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Titanium powders of about 2 mu particle size were subjected to high energy attrition milling in an argon atmosphere. Selecting suitable milling parameters, nanosize (< 100 nm) titanium powders were prepared after 15 h of milling. An average particle size of 35 nm was obtained at 30 h of milling after which the particle size stabilized with continuation of milling to 75 h. The powders after milling for various durations were characterized by TEM, ICP and XRD, and these results are reported and discussed. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:390 / 393
页数:4
相关论文
共 8 条
[1]  
Amarchand S, 2000, ULTRAFINE GRAINED MATERIALS, P33
[2]   MECHANICAL ALLOYING [J].
BENJAMIN, JS .
SCIENTIFIC AMERICAN, 1976, 234 (05) :40-49
[3]  
FECHT HJ, 1996, NANOMATERIALS SYNTHE, P89
[4]  
Gleiter H., 1992, Nanostructured Materials, V1, P1, DOI 10.1016/0965-9773(92)90045-Y
[5]  
Mayo MJ, 1996, INT MATER REV, V41, P85, DOI 10.1179/095066096790326039
[6]  
MOHAN TRR, 1999, ADV POWER METALLURGY, V1, P159
[7]  
Suryanarayana C, 1999, PERG MAT SER, V2, P49
[8]  
SURYANARAYANA C, 1995, INT MATER REV, V40, P41, DOI 10.1179/095066095790151106