共 22 条
Fabrication of 1D nanofluidic channels on glass substrate by wet etching and room-temperature bonding
被引:31
作者:
He, Qiaohong
[1
]
Chen, Shuang
[1
]
Su, Yuan
[1
]
Fang, Qun
[1
]
Chen, Hengwu
[1
]
机构:
[1] Zhejiang Univ, Inst Microanalyt Syst, Hangzhou 310058, Zhejiang, Peoples R China
基金:
中国国家自然科学基金;
关键词:
Fabrication;
Glass nanofluidic chip;
Room-temperature bonding;
Ion-enrichment and depletion;
D O I:
10.1016/j.aca.2008.08.040
中图分类号:
O65 [分析化学];
学科分类号:
070302 ;
081704 ;
摘要:
In this paper, a simple and facile technique for fabricating one-dimensional (1D) glass nanofluidic chips was developed. Instead of using expensive nanolithography, the standard UV lithography and wet chemical etching technique was used to fabricate 1D nanochannels on a glass substrate. Smooth channel surfaces were obtained by adding HNO3 into conventional HF-NH4F etching solution. The calibrated etching rate of 3.6 nm min(-1) was achieved using 1.5 x 10(-2) mol L-1 HF-7.5 x 10(-3) mol L-1 NH4F-7.5 x 10(-3) mol L-1 HNO3 as etchant at 40 degrees C. Inter-day preparation gave a R.S.D. of 6.8% in channel depth. The substrate was bonded with a glass cover plate at room temperature. A minimum aspect ratio (depth to width) of 5.0 x 10(-5) for the nanochannels was achieved. The channel depth before bonding was measured by an a-surface profilometer, and the depth uniformity of nanochannels after bonding was demonstrated by cross-section scanning electron microscopy (SEM) analysis. With this technique, we successfully fabricated a nanofluidic device integrating nanochannel with microchannels and demonstrated the ion enrichment-depletion phenomena. (C) 2008 Elsevier B.V. All rights reserved.