Structural changes in silicon anodes during lithium insertion/extraction

被引:1763
作者
Obrovac, MN [1 ]
Christensen, L [1 ]
机构
[1] 3M Co, Elect & Inorgan Technol Ctr, St Paul, MN 55144 USA
关键词
D O I
10.1149/1.1652421
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The structural changes in silicon electrochemically lithiated and delithiated at room temperature were studied by X-ray powder diffraction. Crystalline silicon becomes amorphous during lithium insertion, confirming previous studies. Highly lithiated amorphous silicon suddenly crystallizes at 50 mV to form a new lithium-silicon phase, identified as Li15Si4. This phase is the fully lithiated phase for silicon at room temperature, not Li21Si5 as is widely believed. Delithiation of the Li15Si4 phase results in the formation of amorphous silicon. Cycling silicon anodes above 50 mV avoids the formation of crystallized phases completely and results in better cycling performance. (C) 2004 The Electrochemical Society.
引用
收藏
页码:A93 / A96
页数:4
相关论文
共 11 条
[1]   A Mossbauer effect investigation of the Li-Sn system [J].
Dunlap, RA ;
Small, DA ;
MacNeil, DD ;
Obrovac, MN ;
Dahn, JR .
JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 289 (1-2) :135-142
[2]  
GLADYSHEVSKII G, 1964, SOV PHYS-CRYSTALLOGR, V9, P338
[3]   The crystal structural evolution of nano-Si anode caused by lithium insertion and extraction at room temperature [J].
Li, H ;
Huang, XJ ;
Chen, LQ ;
Zhou, GW ;
Zhang, Z ;
Yu, DP ;
Mo, YJ ;
Pei, N .
SOLID STATE IONICS, 2000, 135 (1-4) :181-191
[4]   Electrochemically-driven solid-state amorphization in lithium-metal anodes [J].
Limthongkul, P ;
Jang, YI ;
Dudney, NJ ;
Chiang, YM .
JOURNAL OF POWER SOURCES, 2003, 119 :604-609
[5]   Electrochemically-driven solid-state amorphization in lithium-silicon alloys and implications for lithium storage [J].
Limthongkul, P ;
Jang, YI ;
Dudney, NJ ;
Chiang, YM .
ACTA MATERIALIA, 2003, 51 (04) :1103-1113
[6]   High capacity, reversible silicon thin-film anodes for lithium-ion batteries [J].
Maranchi, JP ;
Hepp, AF ;
Kumta, PN .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2003, 6 (09) :A198-A201
[7]  
MORRAL FR, 1934, ARK KEMI MINERAL G B, V11, P37
[8]   The formation and properties of amorphous silicon as negative electrode reactant in lithium systems [J].
Netz, A ;
Huggins, RA ;
Weppner, W .
JOURNAL OF POWER SOURCES, 2003, 119 :95-100
[9]   CHEMICAL DIFFUSION IN INTERMEDIATE PHASES IN THE LITHIUM-SILICON SYSTEM [J].
WEN, CJ ;
HUGGINS, RA .
JOURNAL OF SOLID STATE CHEMISTRY, 1981, 37 (03) :271-278
[10]   A room temperature study of the binary lithium-silicon and the ternary lithium-chromium-silicon system for use in rechargeable lithium batteries [J].
Weydanz, WJ ;
Wohlfahrt-Mehrens, M ;
Huggins, RA .
JOURNAL OF POWER SOURCES, 1999, 81 :237-242