Dark-degradation of reactive brilliant blue X-BR in aqueous solution using α-Fe2O3

被引:24
作者
Dang, S. N. [1 ]
Lu, S. X. [1 ]
Xu, W. G. [1 ]
Sa, J. [1 ]
机构
[1] Beijing Inst Technol, Inst Chem Technol, Beijing 100081, Peoples R China
关键词
Catalysis; Oxidation reduction; Powders; X-ray diffraction;
D O I
10.1016/j.jnoncrysol.2008.07.027
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The precursor of Fe2O3 was prepared by chemical precipitation method with sodium hydroxide (NaOH) and iron chloride hexahydrate (FeCl3 center dot 6H(2)O). The samples annealed at different temperature were characterized by means of X-ray diffraction (XRD) and infrared absorption spectroscopy (IR). Degradation of reactive dye in aqueous solution Was used to evaluate the catalytic performance of the Fe2O3. The experiments of degradation had been done in dark place. The experimental results indicated that the catalytic property of the precursor of alpha-Fe2O3 was excellent. The mechanism of the degradation of reactive dye in aqueous Solution was investigated by comparing the data in the absence and presence of oxygen. The precursor of alpha-Fe2O3 annealed at 300 degrees C was the best. The degradation rate of reactive brilliant blue XBR could exceed 95% in 8 m at 25 degrees C when the concentration of the precursor of alpha-Fe2O3 was 0.1 g/L. The mechanism of the catalytic oxidation reaction was investigated by comparing the X-BR catalytic oxidation data in the absence and presence of oxygen. (C) 2008 Elsevier B.V. All rights reserved.
引用
收藏
页码:5018 / 5021
页数:4
相关论文
共 26 条
[1]   NANOCRYSTALLINE ALPHA-FE2O3 SOL-GEL THIN-FILMS - A MICROSTRUCTURAL STUDY [J].
ARMELAO, L ;
GRANOZZI, G ;
TONDELLO, E ;
COLOMBO, P ;
PRINCIPI, G ;
LOTTICI, PP ;
ANTONIOLI, G .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1995, 193 :435-438
[2]   Raschig rings-Fe203 composite photocatalyst activate in the degradation of 4-chlorophenol and Orange II under daylight irradiation [J].
Bandara, J. ;
Klehm, U. ;
Kiwi, J. .
APPLIED CATALYSIS B-ENVIRONMENTAL, 2007, 76 (1-2) :73-81
[3]   Photocatalytic degradation of model textile dyes in wastewater using ZnO as semiconductor catalyst [J].
Chakrabarti, S ;
Dutta, BK .
JOURNAL OF HAZARDOUS MATERIALS, 2004, 112 (03) :269-278
[4]   Kinetic modeling of photocatalytic degradation of Acid Red 27 in UV/TiO2 process [J].
Daneshvar, N ;
Rabbani, M ;
Modirshahla, N ;
Behnajady, MA .
JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 2004, 168 (1-2) :39-45
[5]   Catalytic decomposition of hydrogen peroxide by Fe(III) in homogeneous aqueous solution: Mechanism and kinetic modeling [J].
De Laat, J ;
Gallard, H .
ENVIRONMENTAL SCIENCE & TECHNOLOGY, 1999, 33 (16) :2726-2732
[6]   Magnetic properties of α-Fe2O3 nanoparticle synthesized by a new hydrothermal method [J].
Giri, S ;
Samanta, S ;
Maji, S ;
Ganguli, S ;
Bhaumik, A .
JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2005, 285 (1-2) :296-302
[7]   LOW-TEMPERATURE OXIDATION OF CO OVER GOLD SUPPORTED ON TIO2, ALPHA-FE2O3, AND CO3O4 [J].
HARUTA, M ;
TSUBOTA, S ;
KOBAYASHI, T ;
KAGEYAMA, H ;
GENET, MJ ;
DELMON, B .
JOURNAL OF CATALYSIS, 1993, 144 (01) :175-192
[8]   Microstructural comparison of calcined and uncalcined gold/iron-oxide catalysts for low-temperature CO oxidation [J].
Hodge, NA ;
Kiely, CJ ;
Whyman, R ;
Siddiqui, MRH ;
Hutchings, GJ ;
Pankhurst, QA ;
Wagner, FE ;
Rajaram, RR ;
Golunski, SE .
CATALYSIS TODAY, 2002, 72 (1-2) :133-144
[9]   ENVIRONMENTAL APPLICATIONS OF SEMICONDUCTOR PHOTOCATALYSIS [J].
HOFFMANN, MR ;
MARTIN, ST ;
CHOI, WY ;
BAHNEMANN, DW .
CHEMICAL REVIEWS, 1995, 95 (01) :69-96
[10]   Systematic control of size, shape, structure, and magnetic properties of uniform magnetite and maghemite particles [J].
Itoh, H ;
Sugimoto, T .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2003, 265 (02) :283-295