Optimization of the isolation of nanocrystals from microcrystalline cellulose by acid hydrolysis

被引:1147
作者
Bondeson, D [1 ]
Mathew, A [1 ]
Oksman, K [1 ]
机构
[1] NTNU, Dept Engn Design & Mat, N-7491 Trondheim, Norway
关键词
acid hydrolysis; cellulose nanocrystals; cellulose whiskers; optimization; response surface methodology;
D O I
10.1007/s10570-006-9061-4
中图分类号
TB3 [工程材料学]; TS [轻工业、手工业、生活服务业];
学科分类号
0805 ; 080502 ; 0822 ;
摘要
The objective of this work was to find a rapid, high-yield process to obtain an aqueous stable colloid suspension of cellulose nanocrystals/whiskers. Large quantities are required since these whiskers are designed to be extruded into polymers in the production of nano-biocomposites. Microcrystalline cellulose (MCC), derived from Norway spruce (Picea abies), was used as the starting material. The processing parameters have been optimized by using response surface methodology. The factors that varied during the process were the concentration of MCC and sulfuric acid, the hydrolysis time and temperature, and the ultrasonic treatment time. Responses measured were the median size of the cellulose particles/whiskers and yield. The surface charge as calculated from conductometric titration, microscopic examinations (optical and transmission electron microscopy), and observation of birefringence were also investigated in order to determine the outcome (efficiency) of the process. With a sulfuric acid concentration of 63.5% (w/w), it was possible to obtain cellulose nanocrystals/whiskers with a length between 200 and 400 nm and a width less than 10 nm in approximately 2 h with a yield of 30% (of initial weight).
引用
收藏
页码:171 / 180
页数:10
相关论文
共 24 条
[1]   Plasticized starch/tunicin whiskers nanocomposites.: 1.: Structural analysis [J].
Anglès, MN ;
Dufresne, A .
MACROMOLECULES, 2000, 33 (22) :8344-8353
[2]   Flow properties of microcrystalline cellulose suspension prepared by acid treatment of native cellulose [J].
Araki, J ;
Wada, M ;
Kuga, S ;
Okano, T .
COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 1998, 142 (01) :75-82
[3]  
Araki J, 2000, LANGMUIR, V16, P2413, DOI 10.1021/1a9911180
[4]   Effect of reaction conditions on the properties and behavior of wood cellulose nanocrystal suspensions [J].
Beck-Candanedo, S ;
Roman, M ;
Gray, DG .
BIOMACROMOLECULES, 2005, 6 (02) :1048-1054
[5]   Effect of microcrystallite preparation conditions on the formation of colloid crystals of cellulose [J].
Dong, XM ;
Revol, JF ;
Gray, DG .
CELLULOSE, 1998, 5 (01) :19-32
[6]  
Dufresne A, 1999, ACS SYM SER, V723, P39, DOI [10.1021/bk-1999-0723.ch003, DOI 10.1021/BK-1999-0723.CH003]
[7]   Influence of dextran on the phase Behavior of suspensions of cellulose nanocrystals [J].
Edgar, CD ;
Gray, DG .
MACROMOLECULES, 2002, 35 (19) :7400-7406
[8]   The Young's modulus of a microcrystalline cellulose [J].
Eichhorn, SJ ;
Young, RJ .
CELLULOSE, 2001, 8 (03) :197-207
[9]   POLYMER NANOCOMPOSITES REINFORCED BY CELLULOSE WHISKERS [J].
FAVIER, V ;
CHANZY, H ;
CAVAILLE, JY .
MACROMOLECULES, 1995, 28 (18) :6365-6367
[10]   Thermoplastic nanocomposites filled with wheat straw cellulose whiskers .1. Processing and mechanical behavior [J].
Helbert, W ;
Cavaille, JY ;
Dufresne, A .
POLYMER COMPOSITES, 1996, 17 (04) :604-611