Small-angle X-ray scattering study of gelation and aging of Eu3+-doped sol-gel-derived siloxane-poly(oxyethylene) nanocomposites

被引:16
作者
Dahmouche, K
Carlos, LD
Santilli, CV
de Zea Bermudez, V
Craievich, AF
机构
[1] Univ Estadual Paulista, Inst Quim, BR-14800900 Araraquara, SP, Brazil
[2] Univ Sao Paulo, Inst Fis, BR-01498 Sao Paulo, Brazil
[3] Univ Tras Montes & Alto Douro, Dept Quim, Vila Real, Portugal
[4] Univ Aveiro, Dept Fis, P-3800 Aveiro, Portugal
关键词
D O I
10.1021/jp013826b
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The aggregation, gelation, and aging of urea-cross-linked siloxane-poly(oxyethylene) nanohybrids [(U600)-n] containing two different amounts of europium triflate initially dissolved in an ethanol-water mixture were investigated by in situ small-angle X-ray scattering (SAXS). For both low (n = [O]/[Eu] = 80) and high (n = 25) europium contents, the SAXS intensity was attributed to the formation of siloxane clusters of about 8-11 Angstrom in size. Siloxane cluster formation and growth is a rapid process in hybrids with low Eu contents and slow in Eu-rich hybrids. An additional contribution to the scattering intensity at very low angles was attributed to the formation of a coarse structure level. At this secondary level, the structure can be described as a set of dense domains containing siloxane clusters embedded in a depleted matrix composed of unfolded polymer chains and solvent. By fitting a theoretical function for this model to the experimental SAXS curves, relevant structural parameters were determined as functions of time during the sol-gel transition and gel aging. For hybrids with low europium contents (n = 80), the size of the siloxane clusters remains essentially invariant, whereas the dense segregation domains progressively grow. In hybrids with high doping contents (n = 25), the preponderant structure variation during the first stages of the sol-gel transformation is the slow growth of siloxane clusters. For these hybrids, the segregation of siloxane clusters forming dense domains occurs only during advanced stages of the process.
引用
收藏
页码:4377 / 4382
页数:6
相关论文
共 31 条
[1]  
BEAUCAGE G, 1995, ACS SYM SER, V97, P585
[2]   Efficient luminescent materials made by incorporation of terbium(III) and 2,2-bipyridine in silica/poly(ethylene oxide) hybrid gels [J].
Bekiari, V ;
Lianos, P ;
Judeinstein, P .
CHEMICAL PHYSICS LETTERS, 1999, 307 (5-6) :310-316
[3]   Optimization of the intensity of luminescence emission from silica/poly(ethylene oxide) and silica/poly(propylene oxide) nanocomposite gels [J].
Bekiari, V ;
Lianos, P ;
Stangar, UL ;
Orel, B ;
Judeinstein, P .
CHEMISTRY OF MATERIALS, 2000, 12 (10) :3095-3099
[4]  
Bermudez V. Z., 1998, J ALLOY COMPD, V21, P275
[5]  
BRINKER CJ, 1990, SOL GEL SCI PHYSICS
[6]   White light emission of Eu3+-based hybrid xerogels [J].
Carlos, LD ;
Ferreira, RAS ;
Bermudez, VD ;
Molina, C ;
Bueno, LA ;
Ribeiro, SJL .
PHYSICAL REVIEW B, 1999, 60 (14) :10042-10053
[7]  
Carlos LD, 2000, ADV MATER, V12, P594, DOI 10.1002/(SICI)1521-4095(200004)12:8<594::AID-ADMA594>3.3.CO
[8]  
2-J
[9]   Sol-gel derived urea cross-linked organically modified silicates.: 2.: Blue-light emission [J].
Carlos, LD ;
Bermudez, VD ;
Ferreira, RAS ;
Marques, L ;
Assunçao, M .
CHEMISTRY OF MATERIALS, 1999, 11 (03) :581-588
[10]  
CARLOS LD, IN PRESS ADV FUNCT M