Enhanced thermal stability of a lithiated nano-silicon electrode by fluoroethylene carbonate and vinylene carbonate

被引:231
作者
Profatilova, Irina A. [1 ]
Stock, Christoph [1 ]
Schmitz, Andre [1 ]
Passerini, Stefano [1 ]
Winter, Martin [1 ]
机构
[1] Univ Munster, MEET Battery Res Ctr, Inst Phys Chem, D-48149 Munster, Germany
关键词
Lithium-ion battery; Electrolyte; Thermal stability; Silicon; Fluoroethylene carbonate; Vinylene carbonate; LITHIUM-ION BATTERIES; GRAPHITE NEGATIVE ELECTRODE; TIN-BASED INTERMETALLICS; SURFACE-FILM FORMATION; PC-BASED ELECTROLYTES; LI-ION; ELECTROCHEMICAL PERFORMANCE; ETHYLENE CARBONATE; SOLID-ELECTROLYTE; CHLOROETHYLENE CARBONATE;
D O I
10.1016/j.jpowsour.2012.08.066
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The thermal behavior of the fully lithiated nano-silicon electrode in contact with an 1 M LiPF6 in EC/DEC electrolyte is investigated by differential scanning calorimetry (DSC) in the absence and presence of fluoroethylene carbonate (FEC) and vinylene carbonate (VC) electrolyte additives. In the additive-free electrolyte, intense exothermic reactions commence at approximately 153 degrees C when in contact with LixSi. At contrast, the onset temperature of the thermal runaway is shifted to 200 degrees C and 214 degrees C when the charged LixSi is heated in the presence of FEC and VC in the electrolytes, respectively. The mechanism of this thermal stability improvement by FEC and VC is studied using attenuated total reflection Fourier transform infrared spectroscopy (ATR-FTIR) and by specific measures to design the SEI on the surface of the nano-Si particles. The additives form a robust "primary SEI" on the surface of the LixSi particles during the first charge that is rich in polycarbonate species and stable at elevated temperatures. In addition, the thermal degradation of FEC and VC in the electrolyte solution yields a highly resistive "secondary SEI" on the electrode surface that covers the lithiated silicon electrode (together with the "primary SEI") and protects it from thermal runaway up to 200 degrees C. (C) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:140 / 149
页数:10
相关论文
共 97 条
[1]   Additives-containing functional electrolytes for suppressing electrolyte decomposition in lithium-ion batteries [J].
Abe, K ;
Yoshitake, H ;
Kitakura, T ;
Hattori, T ;
Wang, HY ;
Yoshio, M .
ELECTROCHIMICA ACTA, 2004, 49 (26) :4613-4622
[2]  
[Anonymous], 1980, Infrared Characteristic Group Frequencies
[3]   Nanostructured materials for advanced energy conversion and storage devices [J].
Aricò, AS ;
Bruce, P ;
Scrosati, B ;
Tarascon, JM ;
Van Schalkwijk, W .
NATURE MATERIALS, 2005, 4 (05) :366-377
[4]   IDENTIFICATION OF SURFACE-FILMS FORMED ON LITHIUM IN DIMETHOXYETHANE AND TETRAHYDROFURAN SOLUTIONS [J].
AURBACH, D ;
DAROUX, ML ;
FAGUY, PW ;
YEAGER, E .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1988, 135 (08) :1863-1871
[5]   On the use of vinylene carbonate (VC) electrolyte solutions for Li-ion as an additive to batteries [J].
Aurbach, D ;
Gamolsky, K ;
Markovsky, B ;
Gofer, Y ;
Schmidt, M ;
Heider, U .
ELECTROCHIMICA ACTA, 2002, 47 (09) :1423-1439
[6]   Safety mechanisms in lithium-ion batteries [J].
Balakrishnan, PG ;
Ramesh, R ;
Kumar, TP .
JOURNAL OF POWER SOURCES, 2006, 155 (02) :401-414
[7]  
Balbuena P.B., 2004, Lithium-Ion Batteries: Solid-Electrolyte Interphase
[8]   CHALCOGENOLATES .61. STUDIES ON HEMIESTERS OF CARBONIC-ACID .1. PREPARATION AND PROPERTIES OF MONOMETHYL AND MONOETHYL CARBONATES [J].
BEHRENDT, W ;
GATTOW, G ;
DRAGER, M .
ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE, 1973, 397 (03) :237-246
[9]   Kinetics of Li insertion into polycrystalline and nanocrystalline 'SnSb' alloys investigated by transient and steady state techniques [J].
Besenhard, JO ;
Wachtler, M ;
Winter, M ;
Andreaus, R ;
Rom, I ;
Sitte, W .
JOURNAL OF POWER SOURCES, 1999, 81 :268-272
[10]   Insertion reactions in advanced electrochemical energy storage [J].
Besenhard, JO ;
Winter, M .
PURE AND APPLIED CHEMISTRY, 1998, 70 (03) :603-608