In situ NiK-edge XANES study of the reducibility of Ni in FCC catalysts

被引:13
作者
Bare, SR [1 ]
Modica, FS [1 ]
Ringwelski, AZ [1 ]
机构
[1] UOP LLC, Des Plaines, IL 60017 USA
关键词
catalysis; FCC; Ni K-edge XANES; in situ studies; Ni oxidation state;
D O I
10.1107/S0909049599001089
中图分类号
TH7 [仪器、仪表];
学科分类号
0804 ; 080401 ; 081102 ;
摘要
The majority of the Ni in an aged equilibrated catalyst (ECAT) from the resid UOP fluid catalytic cracking (FCC) unit in the Pertamina EXOR-1 refinery (with 12,000 ppm Ni) is present primarily as a NiAl2O4 phase. No appreciable Ni reduction occurs below 500 degrees C in a flow of H-2. In situ Ni K-edge XANES has been used to follow the reduction kinetics of this NiAl2O4 phase. Reduction in Ha is described by pseudo-second-order kinetics. An apparent activation energy is estimated to be 26 kcal/mol. This value is compared to that of 4.3 kcal/mol for NiO reduction and 32 kcal/mol for NiAl2O4 reduction. Less than 10% of the Ni is estimated to go through a redox cycle in an FCC unit, resulting in a negligible impact on the hydrogen in coke calculation.
引用
收藏
页码:436 / 438
页数:3
相关论文
共 14 条
[1]   NICKEL CONTAMINATION OF FLUIDIZED CRACKING CATALYSTS - A MODEL STUDY [J].
CADET, V ;
RAATZ, F ;
LYNCH, J ;
MARCILLY, C .
APPLIED CATALYSIS, 1991, 68 (1-2) :263-275
[2]  
CAMPAGNA RJ, 1983, OIL GAS J 1031, P128
[4]  
Cimbalo R.N., 1972, OIL GAS J 0515, P112
[5]  
HETTINGER WP, 1983, AM CHEM SOC DIV PETR, V28, P920
[6]   METAL CONTAMINATION OF CRACKING CATALYSTS .1. SYNTHETIC METALS DEPOSITION ON FRESH CATALYSTS [J].
MITCHELL, BR .
INDUSTRIAL & ENGINEERING CHEMISTRY PRODUCT RESEARCH AND DEVELOPMENT, 1980, 19 (02) :209-213
[7]  
NIELSEN RH, 1993, STUD SURF SCI CATAL, V76, P339
[8]   SEPARATING EQUILIBRIUM CRACKING CATALYST INTO ACTIVITY GRADED FRACTIONS [J].
PALMER, JL ;
CORNELIUS, EB .
APPLIED CATALYSIS, 1987, 35 (02) :217-235
[9]   AN ELECTRON-SPECTROSCOPY AND X-RAY-DIFFRACTION STUDY OF NIO/AL2O3 AND NIO-WO3/AL2O3 CATALYSTS [J].
SCHEFFER, B ;
HEIJEINGA, JJ ;
MOULIJN, JA .
JOURNAL OF PHYSICAL CHEMISTRY, 1987, 91 (18) :4752-4759
[10]  
SRIDHAR S, 1994, Z METALLKD, V85, P616